研究了不同聚四氟乙烯(PTFE)微粉质量分数改性聚酮(PK)的力学性能及摩擦磨损性能,并分析了其在不同润滑条件下的摩擦磨损机理。结果表明:填充PTFE微粉后PK的拉伸强度、压缩强度和邵氏硬度下降;在干摩擦条件下,随着PTFE微粉质量分数的增加,PK复合材料的摩擦因数和磨痕宽度呈下降趋势,当PTFE微粉质量分数为6%时,转移膜最连续,磨痕宽度最低,磨损过程以黏着磨损为主;在油润滑条件下,润滑油和PTFE微粉协同作用,PK复合材料的摩擦因数和磨痕宽度均较干摩擦时明显下降。  相似文献   

2.
采用常温机械共混、高温模压的方法,制备了不同质量分数聚四氟乙烯(PTFE)微粉和碳纤维改性的聚醚醚酮(PEEK)复合材料,对其压缩强度、摩擦磨损性能进行了研究,并分析了其磨损后的表面形貌。结果表明:随着PTFE微粉质量分数的增加,PEEK复合材料的压缩强度呈下降趋势,当PTFE微粉质量分数为40%时,其压缩强度下降至60 MPa。随着聚碳纤维质量分数的增加,PEEK复合材料的压缩强度呈上升趋势。随着PTFE微粉和碳纤维质量分数的增加,PEEK复合材料的干摩擦因数和磨痕宽度逐渐下降,当PTFE微粉质量分数为40%时,PEEK复合材料干摩擦因数下降至0.21,其干摩擦磨痕宽度略有上升。随着碳纤维质量分数的增加,PEEK复合材料在油润滑条件下摩擦因数和磨痕宽度较低并略有下降。PEEK复合材料在干摩擦条件下的磨损机制以磨粒磨损为主,伴有疲劳磨损;在油润滑时,摩擦面可形成稳定连续的润滑膜而保持光滑。PEEK复合材料具有较高的压缩强度,摩擦磨损性能良好,可以制作各种滑动轴承、密封圈等特种机械零部件。  相似文献   

3.
利用MM-200型摩擦磨损实验机,考察了纳米TiO2增强超高分子量聚乙烯(UHMWPE)复合材料在生理盐水润滑下,与Co—Cr—Mo合金对摩时的摩擦磨损性能,用光学显微镜观察了材料摩擦表面磨痕形貌。结果表明,适当填充纳米TiO2可提高UHMWPE的硬度,显著降低摩擦系数,增强耐磨性。UHMWPE的磨损主要表现为粘着、犁沟及塑性变形,TiO2-UHMWPE复合材料的磨损表现为轻微疲劳磨损。  相似文献   

4.
采用MPX-2000型销盘式摩擦磨损试验机评价了分别填充氧化铝、Cu粉、石墨、石墨与Cu粉复配的酚醛树脂基复合材料在载荷为100 N、转速为500 r∕min、室温干摩擦条件下的滑动摩擦磨损性能,并分析了磨损后的表面形貌。结果表明,与未填充相比,填充试样的平均摩擦系数和磨损量均有不同程度的降低,其中由石墨、石墨与Cu粉复配填充试样的磨损量显著降低,分别下降80.7%,84.8%。未填充试样磨损表面出现少量被拔出的磨屑纤维,未见明显润滑膜;而填充试样的磨损表面呈现出明显、均匀的润滑膜。填料改变了酚醛树脂基复合材料的磨损机理,增强了复合材料的抗极压承载和促进润滑膜形成能力,提高了复合材料的摩擦磨损性能。  相似文献   

5.
为改善超高分子量聚乙烯(UHMWPE)在海水润滑介质下的耐磨损性能,采用氧化石墨烯(GO)填充与辐照交联对UHMWPE进行改性处理。利用摩擦磨损试验机研究了辐照前后UHMWPE与GO/UHMWPE复合材料在人工海水润滑介质下的摩擦学性能,利用扫描电子显微镜(SEM)与三维表面轮廓仪扫描试样磨痕表面形貌,计算其磨损率,并分析了其摩擦磨损机理。结果表明,在人工海水润滑介质下,GO填充与辐照交联改性处理均略微增加了UHMWPE的摩擦因数,降低了磨损率;二者共同使用可以协同增强UHMWPE的耐磨性能,降低复合材料的摩擦因数与磨损率; GO填充显著提高了UHMWPE的抗磨粒磨损与抗疲劳磨损性能;辐照交联改性处理进一步提高了GO/UHMWPE复合材料的抗磨粒磨损性能。  相似文献   

6.
采用冷压-烧结成型工艺制备了聚苯酯/MoS_2填充聚四氟乙烯复合材料,考察了聚苯酯含量对复合材料力学性能、聚苯酯和MoS_2含量对复合材料与铝合金及其阳极氧化表面摩擦学性能的影响,用扫描电子显微镜观察了复合材料磨损后的表面形貌。结果表明:填充聚苯酯降低了复合材料的拉伸强度和断裂伸长率,提高了球压痕硬度;随着聚苯酯和MoS_2含量的增加,复合材料对铝合金及其阳极氧化表面摩擦因数逐步减小,磨痕宽度降低。  相似文献   

7.
以针状的硅灰石和鳞片石墨为填料,采用冷压—烧结工艺制备了不同填料含量的聚四氟乙烯(PTFE)复合材料,考察了复合材料的摩擦磨损性能,并利用扫描电子显微镜对磨痕和转移膜进行了分析。结果表明,单独填充硅灰石和石墨时,PTFE的磨损率都会随填料含量的增加而降低,硅灰石的作用要强于石墨;但硅灰石会使PTFE的摩擦因数明显增大,而石墨会使PTFE的摩擦因数降低;2种填料提升PTFE耐磨性的作用机理不同,硅灰石在摩擦过程中会在滑动界面区域上逐渐堆积,起到优先承担载荷的作用;而石墨在摩擦过程中会发生片层的滑移与剥离,有助于转移膜的形成;适量的硅灰石(含量为20 %,质量分数,下同)与石墨(含量为5 %或10 %)复合填充能产生协同效应,使PTFE的磨损率进一步降低,耐磨性比未填充的PTFE提高200倍。  相似文献   

8.
通过冷压烧结成型工艺制备了纳米二氧化硅(SiO_2)填充改性聚四氟乙烯(PTFE)复合材料,探究了不同添加比例的纳米SiO_2/PTFE复合材料在不同转速下摩擦磨损情况。采用三维视频显微镜观察了样品的表面磨痕深度,借助扫描电镜观察摩擦表面形貌并分析磨损机理。结果表明,填充纳米SiO_2后的PTFE复合材料其摩擦因数虽有一定程度的升高,但其体积磨损率却大幅降低。且当纳米SiO_2填充质量分数为5%时,复合材料的体积磨损率降到最低,并在转速为80 r/min时较纯PTFE降低了89.5%。观察分析微观形貌发现,随着纳米SiO_2含量的增大,复合材料的磨损机理逐渐由犁耕磨损和黏着磨损向磨粒磨损转变,且当纳米SiO_2填充含量为10%时,出现轻微的疲劳磨损。  相似文献   

9.
采用冷压-烧结成型工艺制备了3种聚四氟乙烯复合材料,制备了3种不同表面质量的45#钢、铝合金及其表面阳极氧化的摩擦对偶件,考察了聚四氟乙烯复合材料与对偶件配副的摩擦磨损性能,用扫描电子显微镜观察了复合材料磨损后的表面形貌。结果表明:金属表面粗糙度Ra、Ry较大,表面接触区域Mr较小时,聚四氟乙烯复合材料干摩擦因数和磨痕宽度较大;金属表面粗糙度Ra、Ry较小,表面接触区域Mr较大时,聚四氟乙烯复合材料干摩擦因数和磨痕宽度较小。金属表面粗糙度Ra、Ry较小,表面接触区域Mr较大时,在干摩擦剧烈磨损阶段,摩擦表面接触区域产生很大的应力和变形,形成微观的赫兹应力分布,导致了聚四氟乙烯复合材料微切削磨损、疲劳磨损、磨粒磨损和黏着磨损。  相似文献   

10.
对3种聚四氟乙烯复合材料与45#钢和表面阳极氧化铝合金配副进行了摩擦性能测试,测定了不同润滑条件下聚四氟乙烯复合材料的摩擦学性能。用扫描电子显微镜观察了聚四氟乙烯复合材料与表面阳极氧化铝合金摩擦磨损后的表面形貌。结果表明:在油润滑条件下,聚四氟乙烯复合材料摩擦因数和磨痕宽度最小,在干摩擦条件下,聚四氟乙烯复合材料摩擦因数最大;在水润滑条件下,聚四氟乙烯复合材料磨痕宽度最大;在油润滑条件下,摩擦表面可形成均匀连续的转移膜和润滑油膜,表面光滑,从而降低了磨损。  相似文献   

11.
It is well established that a wide range of drugs of abuse acutely boost the signaling of the sympathetic nervous system and the hypothalamic–pituitary–adrenal (HPA) axis, where norepinephrine and epinephrine are major output molecules. This stimulatory effect is accompanied by such symptoms as elevated heart rate and blood pressure, more rapid breathing, increased body temperature and sweating, and pupillary dilation, as well as the intoxicating or euphoric subjective properties of the drug. While many drugs of abuse are thought to achieve their intoxicating effects by modulating the monoaminergic neurotransmitter systems (i.e., serotonin, norepinephrine, dopamine) by binding to these receptors or otherwise affecting their synaptic signaling, this paper puts forth the hypothesis that many of these drugs are actually acutely converted to catecholamines (dopamine, norepinephrine, epinephrine) in vivo, in addition to transformation to their known metabolites. In this manner, a range of stimulants, opioids, and psychedelics (as well as alcohol) may partially achieve their intoxicating properties, as well as side effects, due to this putative transformation to catecholamines. If this hypothesis is correct, it would alter our understanding of the basic biosynthetic pathways for generating these important signaling molecules, while also modifying our view of the neural substrates underlying substance abuse and dependence, including psychological stress-induced relapse. Importantly, there is a direct way to test the overarching hypothesis: administer (either centrally or peripherally) stable isotope versions of these drugs to model organisms such as rodents (or even to humans) and then use liquid chromatography-mass spectrometry to determine if the labeled drug is converted to labeled catecholamines in brain, blood plasma, or urine samples.  相似文献   

12.
2001—2002年国外塑料工业进展   总被引:7,自引:0,他引:7  
收集了2001年7月到2002年6月有关国外塑料工业的相关期刊资料,介绍了2001年到2002年国外塑料工业的发展情况,提供了世界各地域塑料原材料的产量及构成比,日本,美国,加拿大,德国,法国,比利时,墨西哥,芬兰,西班牙等国家的树脂产量,消费量及增长率,以及日本,西欧,北美等地区的不同品种塑料原料消费量和增长率统计,按通用热塑性树脂(聚乙烯,聚丙烯,聚苯乙烯,聚氯乙烯,ABS树脂),工程塑料(尼龙,聚碳酸酯,聚甲醛,热塑性聚酯,聚苯醚),通用热固性树脂(酚醛,聚氨酯,不饱和树脂,环氧树脂),特种工程塑料(聚苯硫醚,液晶聚合物,聚醚醚酮)不同品种的顺序,对树脂的产量,消费量及合成工艺,产品应用开发,树脂品种的延伸及应用的进一步扩展等有关技术作了详细的介绍。  相似文献   

13.
2002~2003年国外塑料工业进展   总被引:12,自引:0,他引:12  
收集了2002年7月-2003年6月国外塑料工业的相关期刊资料,介绍了2002年-2003年国外塑料工业的发展情况,提供了世界各大地区塑料的产量、增长率及所占份额,美国、德国、日本、韩国、法国、比利时、中国台湾、加拿大、巴西、西班牙等国家和地区的树脂产量及消费量,各国、各地区塑料原材料的产量、进出口量、国内消费量及人均消费量,以及日本的塑料原材料的生产情况。按通用热塑性树脂(聚乙烯、聚丙烯、聚苯乙烯、聚氯乙烯、ABS树脂)、工程塑料(聚酰胺、聚碳酸酯、聚甲醛、热塑性聚酯、聚苯醚)、通用热固性树脂(酚醛、聚氨酯、不饱和树脂、环氧树脂)、特种工程塑料(聚苯硫醚、液晶聚合物、聚醚醚酮)的品种顺序.对树脂的产量、消费量、供需状况及合成工艺、产品开发、树脂品种的延伸及应用的进一步扩展等有关技术作了详细的介绍。  相似文献   

14.
15.
16.
针对石油钻井钻屑污染物治理的需要,开发了具有新颖结构的多层双锥液固逆流浸洗塔,整体上具有液固两相多级逆流传质浓度分布特征,级内呈现液固流态化良好的混合传递特性。釆用脉冲示踪法进行了颗粒停留时间分布实验研宄,结果显示多釜串联模型符合其结构与流动混合特征,以理论级数N作为模型参数可以很好地表达颗粒物性及操作参数对过程的影响。在研究范围内,内径100mm的24层双锥塔理论级数在6.11~11.0,随液固比增大而增大、随颗粒粒径增大而减小的趋势。该塔在理论级数6.93的操作条件下连续逆流浸洗,钻屑平均停留时间4.23min残留COD浓度77mg·L-1,与6级间歇逆流平衡浸洗钻屑残留COD浓度56 mg.L-1的实验结果相近,为多釜串联模型用于多层双锥塔浸洗传质模型研究与过程放大提供了实验依据。  相似文献   

17.
2009~2010年世界塑料工业进展   总被引:1,自引:0,他引:1  
收集了2009年7月~2010年6月世界塑料工业的相关资料,介绍了2009~2010年世界塑料工业的发展情况,提供了世界塑料产量、消费量及全球各类树脂的需求量及产能情况.按通用热塑性树脂(聚乙烯、聚丙烯、聚苯乙烯、聚氯乙烯、ABS树脂),工程塑料(尼龙、聚碳酸酯、聚甲醛、热塑性聚酯、聚苯醚),特种工程塑料(聚苯硫醚、液晶聚合物、聚醚醚酮),通用热固性树脂(酚醛、聚氨酯、不饱和聚酯树脂、环氧树脂)不同品种的顺序,对树脂的产量、消费量、供需状况及合成工艺、产品应用开发、树脂品种的延伸及应用的进一步扩展等技术作了详细介绍.  相似文献   

18.
2004~2005年国外塑料工业进展   总被引:1,自引:0,他引:1  
收集了2004年7月-2005年6月国外塑料工业的相关资料,介绍了2004年~2005年国外塑料工业的发展情况。提供了世界几大区域塑料的产量、增长率及所占份额;美国、德国、日本、韩国、法国、比利时、印度、西班牙、中国台湾、加拿大、巴西、英国等国家和地区的不同树脂的产量及消费量;各国、各地区塑料原料的产量、进出口量、国内消费量和人均消费量;日本塑料原料的生产情况。按通用热塑性树脂(聚乙烯、聚丙烯、聚苯乙烯、聚氯乙烯、ABS树脂)、工程塑料(聚酰胺、聚碳酸酯、聚甲醛、热塑性聚酯、聚苯醚)、通用热固性树脂(酚醛、聚氨酯、不饱和树脂、环氧树脂)、特种工程塑料(聚苯硫醚、液晶聚合物、聚醚醚酮、聚砜)的品种顺序,对树脂的产量、消费量、供需状况及合成工艺、产品开发、树脂品种的延伸及应用的扩展作了详细的介绍。  相似文献   

19.
20.
建立了测定地球化学样品中包括As、Cr、Ge、V等18种微量、痕量元素的ICP-MS方法。地化试样用HF-HNO3混酸分解后,以1 1 HNO3溶解干渣。由于制样不使用盐酸,避免了Cl对As、Cr、Ge、V的质谱干扰。用国家一级地球化学标准物质GBW 07309制备溶液优化仪器工作参数,并用于校准。方法测定限(6s)为:0.007~6.4μg/g,精密度(RSD%,n=12)为:29%~9.4%,经过国家一级地球化学标准物质的分析验证,结果与标准值吻合。方法已应用于国土资源调查的试样分析。  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号