排序方式: 共有65条查询结果,搜索用时 15 毫秒
21.
22.
23.
据“Iron and Steel Engineer”,1987;64(5)报道,近几年,许多新技术在粗钢到轧制成品的生产过程中起了重要作用。在这方面板坯、大方坯和小方坯的连铸一直很重要,生产热轧板的原料通常是宽800~2200mm厚150~350mm 的板坯,这些板坯在热轧机上 相似文献
24.
据1990年第六届国际钢铁会议报道,1988年6月,日本钢公司YAWATA厂开发了远距离连铸一直接连轧工艺(CC—HDR),把相距较远的连铸机和热轧厂用高温高速保温传送车连接起来,生产过程中出现了一些通常CC—HPR工艺未曾发生的质量问题,从而在夹杂、内部裂纹、中心偏 相似文献
25.
The CCT curves of supercooled austenite were investigated by using THERMECMASTOR-Z simulation machine, test samples refined from 50 kg vacuum induction furnace and two-stage controlled roiling in laboratorial condition. Test results show that influence of cerium (Ce) addition in low sulfur Nb-Ti-Bearing steel is as follows: Ce can increase the transformation point tara and tAr1, enlarge the interval of transformation (tAr3-tAr1) . Ce moves CCT and rightwards , and reduces hardenability. Ce increases bainitic transformation temperature and enlarges curves upwards interval of bainite formation. With higher cooling rates, Ce changes the martensite from coarse strip to fine strip. It decreases Ms, enhances the trend of lath martensitic structure and limits the formation of lamellar crystal. 相似文献
26.
轮胎花纹块撞击路面的噪声研究 总被引:2,自引:0,他引:2
在充分考虑轮胎胎面花纹块形状的基础上,结合声学基本理论,提出花纹块撞击路面噪声的预报模型,并推导出某方向m个花纹块产生的平均声压级计算公式:Lm=201g ρ0mSl3v^2/4ρ0πll2^2利用该公式对145/70R12和165/70R14轮胎花纹块撞击地面的噪声进行了计算。 相似文献
27.
利用数值模拟方法对宽板V形弯曲过程进行研究,确定了相对弯曲半径对应变中性层位置以及变薄系数的影响。结果表明:随着弯曲过程的进行,相对弯曲半径减小,应变中性层内移系数与相对弯曲半径符合指数函数模型,变薄系数与相对弯曲半径符合指数函数模型。 相似文献
28.
通过采用不同含锰量的三种H10Mn2焊丝与焊剂HJ250G组配对16MnDR的埋弧焊试验,验证了随着H10Mn2焊丝锰含量的增加,该焊接接头的低温冲击韧度也随之增大。 相似文献
29.
本文叙述了15CrMoR厚板埋弧焊的焊接工艺评定,并将工艺评定结果应用于产品的焊接,取得了满意的效果。明确了15CrMoR厚板埋弧焊焊接规范参数匹配的重要性。 相似文献
30.