首页 | 官方网站   微博 | 高级检索  
     

废水催化湿式氧化中CuO催化剂的稳定性研究
引用本文:崔迎.废水催化湿式氧化中CuO催化剂的稳定性研究[J].天津化工,2010,24(1):56-59.
作者姓名:崔迎
作者单位:天津渤海职业技术学院,天津,300402
摘    要:以苯酚配水溶液为研究对象,考察负载型CuO催化剂在微型滴流床反应器中连续流工况下的稳定性。结果表明,温度和进水pH值是影响催化剂稳定性的主要因素,高温下催化剂失活速率加快;负载型CuO/γ-Al2O3催化剂在中性进水(pH0=7.00)条件下具有可观的催化活性且可保持连续使用20hr不失活;而在酸性进水(pH0=5.90)条件下,尽管其催化活性较高但失活现象严重。

关 键 词:苯酚  稳定性  pH值

The stability of CuO catalyst used in catalytic wet oxidation for wastewater
CUI Ying.The stability of CuO catalyst used in catalytic wet oxidation for wastewater[J].Tianjin Chemical Industry,2010,24(1):56-59.
Authors:CUI Ying
Affiliation:Tianjin Bohai Vocational Academy;Tianjin 300402
Abstract:Copper oxide supported over γ-alumina was used as catalyst for wet oxidation of aqueous phenol in the TBR.The catalytic activity and stability of CuO/γ-Al2O3 were tested in termed of COD conversion at different reaction temperature and inlet pH.It showed that the catalyst losed its activity more lastly at high temperature.At neutral inlet the catalyst could hold considerable activity within 20h of continuous operation.While the inlet pH was 5.90,the catalyst activity was some more higher but its stability was weaker.
Keywords:phenol  stability  pH  
本文献已被 CNKI 维普 万方数据 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号