A carbon-13 method for evaluating degradation of starch-based polymers
Authors:Martha L Sykes  Hsueh-Wen Yeh  Ian F West  R W Gauldie  Charles E Helsley
Affiliation:(1) Hawaii Institute of Geophysics and Planetology, School of Ocean and Earth Science and Technology, University of Hawaii at Manoa, 2525 Correa Road, 96822 Honolulu, Hawai
Abstract:A new method for evaluating biodegradability of starch-based and certain other polymer blends uses the pre- and postexposure stable carbon isotope composition of material coupled with weight loss data to determine which components have degraded. The naturally occurring stable isotope of carbon.13C, is enriched in corn starch (delta13C, approx. –11permil) compared to petroleum-derived synthetic polymers (delta13C, approx. –32permil). Results on starch-synthetic polymer blends indicate that the delta13C signatures of these blends are near-linear mixtures of their component delta13C. Values of a delta13C for starch-synthetic polymer blends exposed to biologically active laboratory soil and artificial seawater conditions are depleted in13C compared to unexposed samples, suggesting loss of the starch component. Combined with weight loss data for the exposed samples, the delta13C values are statistically consistent with models requiring loss of the soluble component glycerin, followed by loss of starch, then petrochemical polymer, or simultaneous loss of starch and petrochemical polymer. Replicate delta13C analyses of starch-synthetic polymer blends increase the statistical power of this relatively inexpensive, accessible technique to discriminate between degrading components.
Keywords:Biodegradation  stable isotope  starch-based polymer  carbon-13
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号