Abstract: | Conclusion Alloy KhN35VTYu has high values of u, 0.2, and a0.25 at normal and cryogenic temperatures after hardening at 1050°C for 3 h in air and aging at 700°C for 3–8 h. The alloy is not sensitive to stress concentration. Increasing the hardening temperature to 1200°C leads to a significant decrease in the values of 0.2 and a0.25.VNIIÉM, IMASh. Translated from Metallovedenie i Termicheskaya Obrabotka Metallov, No. 5, pp. 28–29, May, 1991. |