小方坯连铸机漏钢原因分析及对策
引用本文:江小敏.小方坯连铸机漏钢原因分析及对策[J].江西冶金,2008,28(5).
作者姓名:江小敏
作者单位:新余钢铁有限责任公司,江西,新余,338001
摘    要:通过对小方坯连铸机漏钢现象进行分析,找出结晶器铜管锥度及装配不合理,冷却不均匀等是产生漏钢的重要原因,并采取有效措施,使漏钢率降低,取得良好效果.

关 键 词:连铸  小方坯  漏钢  措施

Causes Analysis and Countermeasures of Breakout for Billet Continuous Caster
JIANG Xiao-min.Causes Analysis and Countermeasures of Breakout for Billet Continuous Caster[J].Jiangxi Metalllurgy,2008,28(5).
Authors:JIANG Xiao-min
Affiliation:JIANG Xiao-min (Xinyu Iron , Steel Co.Ltd.,Xinyu 338001 Jiangxi,China)
Abstract:Through phenomenon analysis of breakout for billet continuous caster,main causes of breakout such as unreasonable mould copper tube taper and assembling,uneven cooling and so on were found.The breakout ratio was reduced by taking effective measures,and a good effeet had been achieved.
Keywords:continuous  small billet  breakout  measure  