Development of high-content extra fine count blended yarn with rabbit hair and silk
ZHANG Jin.Development of high-content extra fine count blended yarn with rabbit hair and silk[J].Shanghai Textile Science & Technology,2006,34(1):48-50.
Authors:ZHANG Jin
Abstract:Due to the fatal weaknesses of rabbit hair which leads to poor spin ability, low strength, lager static and being easy to break and to fall off when in processing and wearing, rabbit hair is hard to develop thin product. By using domestic wool and cotton spinning equipment in a combined way, choosing silk as blending material and adopting 40/60 silk-rabbit hair blending ratio as well as by improving equipment parameters and processing technology, high-content extra fine rabbit hair and silk blended yarn of good evenness and few hairiness is made, which can be used for weaving and knitting.
Keywords:spinning  blended yarn  rabbit hair  real silk