渣成分对冶炼28MnCr5齿轮钢时CaO-SiO2-Al2O3-MgO精炼渣系熔点的影响
引用本文:梁娜,吴德发,翟正龙,张利平.渣成分对冶炼28MnCr5齿轮钢时CaO-SiO2-Al2O3-MgO精炼渣系熔点的影响[J].特殊钢,2012,33(4):10-12.
作者姓名:梁娜  吴德发  翟正龙  张利平
作者单位:1. 莱芜钢铁集团有限公司特钢事业部,莱芜,271104
2. 莱芜钢铁集团有限公司宽厚板厂,莱芜,271104
摘    要:以28MnCr5齿轮钢(/%:0.28C、0.09Si、0.70Mn、0.015P、0.027S、0.95Cr)50 t电弧炉-LF-VD的生产过程为对象,利用热力学计算软件FactSage,研究CaO-SiO2-Al2O3-MgO精炼渣系中不同成分比例对其熔点的影响,找出最佳的比例使夹杂物控制在低熔点区域,以便于去除。结果表明,(CaO)/(SiO2)≤1时,低熔点区域占总相图面积的百分比较大;当CaO含量为30%时,低熔点区域占总相图面积的百分比达到所有的最大值,为53.2%;4组元最佳配比为(%)30CaO-30SiO2-25Al2O3-15MgO。

关 键 词:28MnCr5齿轮钢  精炼渣  相图  低熔点

Effect of Slag Ingredient on Melting Point of CaO-SiO2-Al2O3-MgO Refining Slag Series for Gear Steel 28MnCr5 Steelmaking
Liang Na , Wu Defa , Zhai Zhenglong , Zhang Liping.Effect of Slag Ingredient on Melting Point of CaO-SiO2-Al2O3-MgO Refining Slag Series for Gear Steel 28MnCr5 Steelmaking[J].Special Steel,2012,33(4):10-12.
Authors:Liang Na  Wu Defa  Zhai Zhenglong  Zhang Liping
Affiliation:1 (1 Special Steel Division;2 Heavy Plate Plant,Laiwu Iron and Steel Group Co Ltd,Laiwu 271104)
Abstract:Based on the process of 50 t EAF-LF-VD for gear steel 28MnCr5(/%:0.28C,0.09Si,0.70Mn, 0.015P,0.027S,0.95Cr),the effect of proportion of each ingredient in slag on melting point of CaO-SiO2-Al2O3-MgO refining slag series has been studied by using thermodynamic calculation software FactSage,to get optimum proportion of ingredients in order to control the inclusions in low melting point region and remove out.Results show that as(CaO)/(SiO2)≤1,the percentage of low melting point region to whole phase diagram area is larger and as CaO content in slag(CaO) is 30%,the percentage of low melting point region to whole phase diagram area is maximum i.e.53.2%;the optimum ingredient of quaternary refining slag series is(/%) 30CaO-30SiO2-25Al2O3-15MgO.
Keywords:Gear Steel 28MnCr5  Refining Slag  Phase Diagram  Low Melting Point