基金项目:“十三五”国家重点研发计划(2018YFD0600303);北京市自然科学基金(8151003)
摘    要:以西南传统民居穿斗式木结构穿销中节点为研究对象,设计制作了2个足尺横向中节点和2个足尺纵向中节点模型试件,分别对两类节点进行单调加载和低周往复加载试验,得到两类节点的破坏模式、抗弯承载力、抗弯刚度、延性和耗能能力.结果 表明:横向中节点主要在榫卯挤压区域发生嵌压塑性变形以及在木销受荷区域发生弯剪变形,纵向中节点易在榫颈...

关 键 词:穿斗式木结构  中节点  抗弯性能  抗震性能
收稿时间:2020/12/2 0:00:00

Experimental study on the moment-resisting performance of interior joints with wooden peg
GUO Ting,YANG N,ZHOU Haibin,WANG Shuangyong.Experimental study on the moment-resisting performance of interior joints with wooden peg[J].Journal of Civil and Environmental Engineering,2022,44(2):83-90.
Authors:GUO Ting  YANG N  ZHOU Haibin  WANG Shuangyong
Affiliation:School of Civil Engineering, Beijing Jiaotong University, Beijing 100044, P. R. China;Research Institute of Wood Industry, Chinese Academy of Forestry, Beijing 100091, P. R. China
Abstract:In order to study the moment-resisting performance and seismic behavior of the interior joints with wooden peg of Chuan-Dou type wooden frame, two full-scale interior beam-column joint specimens of transverse frame and two that of longitudinal frame were designed and fabricated. Monotonic loading and low cyclic loading tests were carried out on the two types of joints, respectively. The failure mode, moment-resisting capacity, flexural stiffness, ductility and energy dissipation of the two types of joints were obtained. The results showed that the failure mode of transverse interior joint was the embedment plastic deformation on the mortise and tenon contacting area as well as the bending-shear combined deformation of wooden peg, while longitudinal interior joint was broken off at the neck of tenon. The initial stiffness of the transverse interior joint was higher than that of the longitudinal interior joint. The moment-resisting capacity of transverse interior joint could reach two times of that of longitudinal interior joint. The hysteretic loops of the two types of joint exhibited obvious squeezing and slip. The energy dissipation of the transverse interior joint was higher than that of the longitudinal interior joint. Both the two types of joint exhibited good deformation capacity, the transverse interior joint exhibited good ductility, while the longitudinal interior joint exhibited poor ductility.The longitudinal interior joint in the frame is the weakest part and need to be noted on the safety maintenance of the Chuan-Dou type wooden frame structure.
Keywords:Chuan-Dou type wooden frame  interior joint  moment-resisting performance  seismic behavior