棒状Ni/CuO-ZnO的制备及其反应吸附脱硫性能研究
引用本文:高乾朔,王海彦,康蕾.棒状Ni/CuO-ZnO的制备及其反应吸附脱硫性能研究[J].石油炼制与化工,2015,46(11):70-73.
作者姓名:高乾朔  王海彦  康蕾
作者单位:辽宁石油化工大学化学化工与环境学院
摘    要:采用水热合成法制备了棒状CuO-ZnO复合氧化物,采用等体积浸渍法制备了Ni/CuO-ZnO吸附剂,采用TG、SEM,XRD,BET方法进行了表征。在固定床反应器中进行了吸附剂的反应吸附脱硫性能评价。结果表明:制备的CuO-ZnO复合氧化物呈棒状结构,复合氧化物适宜的焙烧温度为500 ℃;Cu的掺杂有效改进了反应吸附剂的脱硫性能,Cu的最佳掺杂量(w)为10%,掺杂Cu后脱硫率较Ni/ZnO平均脱硫率提高17.4百分点,且能延长有效脱硫时间,吸附剂在45 h左右仍能保持较高的脱硫活性。

收稿时间:2015-04-02
修稿时间:2015-04-20

STUDY ON PREPARATION AND REACTIVE ADSORPTION DESULFURIZATION PERFORMANCE OF RODLIKE Ni/CuO-ZnO
Abstract:The rodlike CuO-ZnO complex oxides were prepared by hydrothermal synthesis method. The adsorbents of Ni/CuO-ZnO were prepared by incipient-wetness impregnation method. The complex oxides and the adsorbents were characterized by TG,XRD, SEM and BET techniques. The performance of reactive adsorption desulfurization for thiophene was evaluated in a fixed bed reactor. The results indicate that the suitable calcination temperature for composite oxides and Ni/CuO-ZnO is 500 ℃. The doping of Cu effectively improves the reactive adsorption desulfurization performance, and the adsorbent with 10% CuO shows the best desulfurization activity, 17.4 percentage points higher than the reference Ni/ZnO. And the adsorbent with Cu doping is more stable, the adsorbent still remain high desulfurization activity in 45 hour.
Keywords:
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《石油炼制与化工》浏览原始摘要信息
点击此处可从《石油炼制与化工》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号