Compression Testing of Ti-6Al-4V in the Temperature Range of 303-873K |
| |
Authors: | K. Srinivasan P. Venugopal |
| |
Affiliation: | a Department of Metallurgical and Materials Engineering, National Institute of Technology Karnataka, Surathkal, Indiab Materials Forming Laboratory, Department of Metallurgical and Materials Engineering, Indian Institute of Technology, Madras, Chennai, India |
| |
Abstract: | Compression testing of Ti-6Al-4V alloy has been carried out at temperatures between 303 K to 873 K. To prevent embrittlement due to atmospheric oxygen and nitrogen, the samples were given a glass coating, which also acts as a lubricant simultaneously. Dynamic Strain Aging was observed to occur in the temperature range of 600 K to 800 K. Below 600 K stresses were high. Warm working has to be done above 800 K but below 1163 K (0.6 Tm where Tm = 1940 K) which is the recrystallization temperature. Based on these conclusions, warm extrusion has been successfully carried out in the Materials Forming Laboratory of I.I.T., Madras, Chennai, India. |
| |
Keywords: | Compression Dynamic strain aging Flow properties Temperature Ti-6Al-4V Warm working Work hardening |
本文献已被 InformaWorld 等数据库收录! |
|