排序方式: 共有125条查询结果,搜索用时 0 毫秒
1.
2.
The microstructures and properties of Cu-8.0Ni-1.8Si alloy subjected to different heat treatments were examined by mechanical and electrical properties measurements, optical and transmission electron microscopes observation. The results show that the precipitation process during aging can be accelerated by the cold deforming before aging. As the Cu-8.0Ni-1.8Si alloy is subjected to solution treatment at 970 ℃ for 4 h, cold rolling to 60% reduction, and then aging at 450 ℃ for 60 min, its properties are σb=1 050 MPa, σ0.2=786 MPa, δ=3.2% and conductivity 27.9%(IACS). The strengthening mechanisms of the alloy include spinodal decomposition strengthening, ordering strengthening and precipitation strengthening. The precipitation of the alloy is nano-scale Ni2Si phase. 相似文献
3.
我局新建的3500m3/h大型绞吸船新海豚轮运行稳定和施工高效,都离不开变频驱动技术的应用。本文分别对比绞刀的变频和液压驱动、水下泵的变频和高压F-D驱动的性能,分析变频驱动使用中存在的问题以及解决办法,展望了变频驱动在绞吸船上的应用前景。 相似文献
4.
潘志勇 《湖南工业职业技术学院学报》2008,8(1):3-5
通过对较高Cu含量的铝合金微观组织的观察,在研究半固态加工的Al-10%Cu、Al-20%Cu和Al-40%Cu合金中初生α-Al枝晶、共晶晶粒和初生θ相的形貌、尺寸的变化规律之后。对半固态加工Al-Cu合金的微观组织形成进行了分析,指出了其形成机理。 相似文献
5.
潘志勇 《中国新技术新产品》2014,(9):134-134
文章积极探析氧化沟工艺处理城市生活污水的流程,希望可以以此强化的应用效果,给予实践工作以指导意见和建议。 相似文献
6.
7.
8.
9.
圆螺纹套管接头发生脱扣主要与产品设计加工、材质性能、上扣扭矩或上扣位置以及现场操作等方面的因素有关。近几年,国产套管质量有了很大的提高,然而圆螺纹套管接头滑脱事故仍时有发生,导致了较大的经济损失和安全事故的发生。针对一起圆螺纹套管脱扣事故,采用理论分析与试验相结合的方法,对脱扣套管和接箍进行了宏观分析和材质理化性能试验,并对同批次套管试样进行了螺纹参数测量和实物拉伸模拟试验,最后对试验结果进行了综合分析。结果表明:现场上扣时夹持接箍位置错误、现场端上扣不到位是导致该套管脱扣失效的主要原因。 相似文献
10.
对带有腐蚀坑的φ127mm API钻杆内、外螺纹端钻杆内加厚过渡带管体刺漏前后的速度场和压力场进行模拟。结果表明:流场的诱导对存在腐蚀坑的钻杆管体的刺漏失效起着承上启下的作用,腐蚀坑越深,腐蚀坑底的湍动能越大;入口流量增大,腐蚀坑部位的剪切应力越大,钻杆的刺漏越容易发生;在相同的井况条件下,钻杆内螺纹接头端内加厚过渡带比外螺纹端刺漏失效多的原因与流场的Bernoulli效应密切相关;当钻杆内加厚过渡带管体存在刺孔时,钻杆发生刺漏失效与相应位置的环空压力密切相关,在环空压力小的位置刺漏时的湍动能和最大速度最大。 相似文献