Nano-F /Fe^3+/TiO2 particles were prepared by hydrolysis of tetrabutyl titanate in a mixed CF3COOH-Fe(NO3)3-H2O solution. The photocatalytic decomposition of methylene blue in aqueous solution was used as a probe to evaluate their photocatalytic activities. The powders were characterized by X-ray diffraction (XRD), energy dispersion X-ray spectrum (EDS) and Brunauer-Emmett-Teller (BET) surface area analysis. The results show that F- and Fe^3+ are doped into TiO2. The F^- and Fe^3+ doping can help to enhance the nano-TiO2 photocatalytic activity greatly. The appropriate codoping conditions for F-Fe are n(F)/n(TiO2)=2%, n(Fe)/n(TiO2)=0.05%, and the degradation rate of methylene blue at l h is improved from 73.2% to 87.5%. The codoped nano-F /Fe^3+/TiO2 particles have higher BET specific surface area, smaller crystallite size and higher photocatalytic activity than those of undoped TiO2 particles. 相似文献
2.
使用混合溶剂热法,以1-己基-3-甲基咪唑溴盐离子液体([Hmim]Br)和Bi(NO3)3·5H2O为反应物,乙二醇水溶液为溶剂,制备了BiOBr微球和纳米片。利用X射线衍射(XRD)、扫描电镜(SEM)、紫外可见漫反射(UV-Vis)以及N2吸附-脱附等手段对其进行了物相和结构的表征。在可见光照射下,以罗丹明B(RhB)为目标污染物,研究了离子液体存在下,溶剂组成对BiOBr光催化活性的影响。结果表明,当乙二醇与水的比例为3∶1~1∶1时所制备的BiOBr纳米片具有最高的光催化活性;同时,BiOBr纳米片光催化剂稳定性良好,循环使用8次后光催化活性基本稳定。 相似文献
3.
4.
AM/SA反相微乳液聚合反应动力学研究 总被引:2,自引:0,他引:2
以油酸失水山梨醇酯Span80和壬基酚聚氧乙烯醚OP-10为乳化剂,白油为连续介质,高活性过氧化二碳酸(2-乙基已基)酯(EHP)为引发剂,进行了丙烯酰胺/丙烯酸钠(AM/SA)反相微乳液共聚合反应。研究了单体总浓度[M],引发剂浓度[I],乳化剂浓度[E]对AM/SA反相微乳液聚合速率Rp和共聚物分子量M^-v的影响规律,得到Rp∞[M]^m[I]^0.65[E]^0.34,M^-v∞[M]^n[I]^-0.30[E]^-1.08,其中当[M]=3.21mol/L-6.42mol/L时,m=2.34,n=0.68,当[M]=1.28mol/L-3.33mol/L时,m=1.61,n=0.58,比较了不同单体浓度范围内AM/SA反相微乳液聚合速率。 相似文献
5.
催化裂化汽油光化学氧化脱硫 总被引:2,自引:0,他引:2
以水为萃取剂、空气中的O2为氧化剂、500W高压汞灯为紫外光光源,研究了催化裂化(FCC)汽油光化学氧化反应的机理和氧化产物,考察了反应条件对FCC汽油脱硫率的影响。实验结果表明,FCC汽油中的极性含硫化合物首先部分溶于水相中,然后在水相中被氧化。在空气通入量为150mL/min、水与FCC汽油的体积比为1.0的条件下,反应5h后FCC汽油脱硫率达40.6%,加入0.45g4A分子筛作为O2的吸附剂后FCC汽油脱硫率提高到70.2%。FCC汽油的光化学氧化反应为一级动力学反应,加入4A分子筛时的反应速率常数为0.217 4h-1,半衰期为3.18h。FCC汽油光化学氧化反应的主要产物为亚砜和砜,并进一步生成CO2、草酸、SO24-等。 相似文献