排序方式: 共有43条查询结果,搜索用时 0 毫秒
1.
Microstructures and evolution mechanism of highly undercooled Ni-Pb hypermonotectic alloy 总被引:1,自引:0,他引:1
The microstructures and evolution mechanism of the undercooled Ni-20%Pb(molar fraction) alloy were investigated systematically by high undercooling solidification technique. The experiment results indicate that the morphology of α-Ni phase and the distribution of Pb element in undercooled Ni-20% Pb alloys change with the in-crease of undercooling. The main evolution mechanisms of α-Ni are dendrite remelting and recrystallization. Pb phase in the microstructure of Ni-20% Pb hypermonotectic alloy originates from L2 phase separated from the parent melt during the cooling process through immiscible gap and L2 phase formed at the temperature of monotectic trans-formation. The solubility of Ph element in α-Ni phase under high undercooling condition is up to 5.83% which is ob-viously higher than that under equilibrium solidification condition. The real reason that causes the solubility difference is distinct solute trapping. 相似文献
2.
3.
Y和Ce的同时加入使镁合金获得了优异的阻燃效果,实现了镁合金在大气条件下的无保护熔炼。AES和XRD表面分析结果表明,Mg-Y-Ce阻燃镁合金在高温下暴露于大气中时,合金表面会生成一层以Y2O3为主的氧化膜。干燥空气中,Mg-3Y-4.5Ce合金在773, 873和973 K下氧化时,其氧化动力学曲线遵循立方规律。基于高温氧化热力学,详细分析了Mg-Y-Ce合金在高温下的选择性氧化机制,并从电化学角度探讨了Y2O3膜的半导体特性及其对镁合金基体进一步氧化的阻碍机制 相似文献
4.
5.
6.
7.
Cu-Cr-Zr合金是电气化铁路接触网装备的重要材料,其抗拉强度和导电率性能要求较高。采用高频熔炼、铜模快冷、固溶处理、冷轧和退火处理制作了Cu-Cr-Zr合金样品,分析了其显微组织、抗拉强度和导电率之间的关系。在铜晶粒内部和晶界上析出的第二相Cu5Zr和其他多元化合物是Cu-Cr-Zr合金获得高强度的主要原因。固溶体中的Cr、Zr溶质含量是影响合金电阻率的主要因素,纳米及亚微米级的第二相可使合金获得较好的强度和导电性。冷轧后试样经过450℃、550℃退火处理,发现550℃退火处理后Cu-0.7Cr-0.4Zr合金的抗拉强度可达550MPa,导电率达82.5%IACS。 相似文献
8.
9.
连续输送技术专业委员会第四届年会于1991年9月25~28日在沈阳市召开,参加会议的有工厂、用户、设计研究所和大专院校共56个单位的80名代表。会上宣读和交流论文40余篇。其中“直线电机驱动带式输送机的试验研究”、“吊挂管状带式输送机”、“面控制式胶带纵向撕裂自动检测装置的研制”、“长距离胶带机电气控制的特点”等均反映了我国连续输送技术最新研 相似文献
10.