排序方式: 共有72条查询结果,搜索用时 0 毫秒
1.
2.
贺海燕 《武汉理工大学学报(材料科学英文版)》2009,24(3):359-362
Fatigue-free Bi3.2La0.8Ti3O12 ferroelectric thin films were successfully prepared on p-Si (100) substrates using metalorganic solution deposition process. The orientation and formation of 5-layers thin films
were studied under different processing conditions using XRD. Experimental results indicate that increase in annealing time
at 700 °C after preannealing for 10 min at 400 °C can remarkably increase (200)-orientation of the films derived from the
precursor solutions with two contents of citric acid. Meanwhile, high content of citric acid increases the film thickness
and is conducive to the a-orientation of the films with the preannealing, and low concentration of the solution is conducive to the c-orientation of
the films without the preannealing. 相似文献
3.
论述了由不同制备工艺获得的Fe2O3陶瓷及各种添加剂下表面羟基和吸附氧的形成和性质,分析了表面羟基和吸附氧的酸碱性对气湿特性的影响。 相似文献
4.
超细BaTiO3粉体制备的研究进展 总被引:3,自引:0,他引:3
综合评述了超细酸钡BaTiO3粉体制备目前采用的各种方法,包括共沉淀法、微乳液法、柠檬酸法、草酸盐法、水热法、溶液热合成法、Sol-gel法和金属有机物热解法和有机盐-氢氧化物法.评述了目前对先驱体溶液化学对溶胶的形成、溶胶凝胶转变、粉体的形成影响以及晶粒尺寸和粒子尺寸与粉体结构的关系. 相似文献
5.
6.
7.
以氯化钐为起始原料,采用溶胶-凝胶法在玻璃和Si(100)基板上制备了Sm2O3光学薄膜,在300~800℃对薄膜进行1~3 h热处理.采用X射线衍射、原子力显微镜和紫外-可见自记式分光光度计等对薄膜的结晶取向、显微结构和光学性能进行了表征.结果表明:Sm2O3薄膜在玻璃基板和Si(100)基板上均表现出沿(311)晶面定向生长的特征;Si基板更有利于生长致密而且结晶良好的薄膜;所制备的薄膜对紫外线有强烈吸收作用,而对可见光有较好的透过作用,随着热处理温度的升高,薄膜结晶性变好,取向性增强,光吸收性能增强,薄膜的禁带宽度减小. 相似文献
8.
应用Sol-gel法成功合成了纳米SrTiO3粉体。酞酸丁酯和氯化锶为金属离子源,先驱体以甲醇为溶剂、柠檬酸为螯合剂、乙酰丙酮为稳定剂、聚乙二醇和聚乙烯醇为模板。干先驱体经700℃1h烧成后得到纯的SrTiO3粉体。研究了表面活性剂对粉体的粒子尺寸和形貌的影响。合成粉体的聚乙二醇诱导了均匀的较小的圆形粒子。聚乙烯醇则使合成粉体为较大尺寸的长板柱状的粒子。 相似文献
9.
应用sol-gel法成功地低温合成了超细BaFe12O19磁粉。先驱体氢氧化物在醇:水比为1:1.7、Ba^2+和Fe^3+以的离子摩尔比为1.15:12的溶胶溶液中(以氢氧化钠NaOH为沉淀剂)制得。采用两步热处理法,先驱体氢氧化物在300℃预热处理1h,再在800℃热处理5h,X射线衍射分析(XRD)分析表明形成了BaFe12O19磁性粒子,粒子尺寸为42.0nm,接近理论单畴尺寸40nm。 相似文献