研究了聚醚型聚氨酯橡胶/氯丁橡胶共混物复合交联体系及其对共混硫化胶物理机械性能的影响;探讨了聚氨酯橡胶/氯丁橡胶共混胶料的硫化特性,共混硫化胶的力学性能、耐热老化性能和动态力学性能.结果表明:硫黄/MgO体系能够很好地硫化PUR/CR共混胶;当共混胶中PUR用量在0~100份范围内,共混胶的焦烧时间和正硫化时间均先减小后增加,最小转距和最大转距都降低;拉伸强度、撕裂强度和硬度均随PUR用量的增加而增加.拉断伸长率在PUR用量为40份时最大;共混硫化胶的耐热老化性能随着PUR用量的增加而增加,其拉仲强度保持率和拉断伸长率保持率呈上升趋势;动态力学研究表明,PUR和CR有很好的相容性,玻璃化温度随着PUR用量的增加而降低.  相似文献   

2.
研究了不饱和聚醚型聚氨酯橡胶(PUR)和氯丁橡胶(CR)的共混比、硫黄用量、炭黑种类及用量、软化刺种类及用量以及防老剂诸因素对PUR/CR共混物耐热老化性能的影响.结果表明,当PUR与CR的质量比20/80、硫黄用量1.0~1.5份、炭黑选用N220且其用量40份、软化荆选用古马隆树脂且用量5份以及选用防老荆RD时,可以得到耐热老化性能较好的PUR/CR共混物.  相似文献   

3.
刘凉冰 《橡胶工业》2018,65(3):351-355
介绍混炼型聚氨酯(MPU)橡胶的研究现状,讨论影响MPU橡胶性能的因素。与聚醚型MPU橡胶相比,聚酯型MPU橡胶的耐低温性能好,耐光性能稳定,耐磨性能优异,添加水解稳定剂后耐水性能大大提高。与硫黄硫化的MPU橡胶相比,硫化剂DCP硫化的MPU橡胶压缩永久变形较小。温度升高,MPU橡胶的物理性能、耐老化性能、耐水性能和耐湿性能均下降。添加增塑剂后MPU橡胶的物理性能和耐磨性能下降,耐低温性能改善。  相似文献   

4.
王孝忠 《粘接》1992,13(3):24-26
常用的金属底胶,使聚醚型聚氨酯橡胶与钢粘合的剥离强度为14.1~16kN/m。采用本金属底胶,能使聚醚型聚氨酯橡胶与黄铜、不锈钢的剥离强度提高到28kN/m以上,与黄铜、不锈钢、硬铝、锻铝的抗拉强度达9.3MPa以上。测试样件基本上均为橡胶内聚破坏。该底胶已成功地应用于水声换能器中,经五年多生产、使用考验,水密性良好。  相似文献   

5.
钟达飞  鲍俊杰  谢伟  许戈文 《中国涂料》2007,22(3):27-28,35
主要探讨了端羟基聚丁二烯橡胶(HTPB)对水性聚氨酯(WPU)耐水性、力学性能、胶膜手感的影响,以及不同交联剂对胶膜的影响。  相似文献   

6.
浇注型聚氨酯橡胶   总被引:3,自引:0,他引:3  
  相似文献   

7.
过氧化物硫化聚醚型聚氨酯混炼橡胶力学性能的研究   总被引:2,自引:0,他引:2  
研究了过氧化物过氧化二异丙苯(DCP)、双叔丁基过氧化异丙基苯(BIPB)和补强剂(炭黑或白炭黑)对聚醚型聚氨酯混炼橡胶力学性能的影响,讨论了DCP和补强剂用量变化及不同硫化条件对混炼橡胶力学性能的影响。结果表明,DCP硫化混炼胶定伸应力高,永久变形小;BIPB硫化混炼胶硬度和强度高;当DCP用量在1.6份时,混炼胶拉伸强度和撕裂强度最高;提高补强剂用量,混炼胶硬度和定伸应力增加,拉伸强度变化不明显,但永久变形变大。  相似文献   

8.
用多因素回归分析法设计实验,研究炭黑N330和硫黄用量对混炼型聚氨酯(MPU)胶料性能的影响。结果表明:在本工作设定的范围内,当硫黄用量固定时,随着炭黑N330用量增大,MPU胶料的硬度、100%定伸应力、撕裂强度和DIN磨耗体积提高,拉伸强度、拉断伸长率和回弹值降低;当炭黑N330用量固定时,随着硫黄用量增大,MPU胶料的硬度没有明显变化,拉伸强度略降低,拉断伸长率和撕裂强度先提高后降低,回弹值下降;当炭黑N330用量较低时,DIN磨耗体积随着硫黄用量增大而增大;根据回归分析法建立的数学模型可以较准确地预测MPU胶料各项性能随硫黄和炭黑用量变化而变化的趋势。  相似文献   

9.
五十年代由联邦德国拜耳(Beyer)公司首先研制的聚酯型聚氨酯浇注橡胶,于六十年代获得迅速发展,山西省化工研究所七十年代初研制成功了这种橡胶,这种材料经不断改进,使用范围不断扩大,先后在国内十多个生产厂家推广。  相似文献   

10.
邱劲东 《橡胶科技》2018,16(11):27-30
进行混炼型耐磨聚氨酯橡胶的配方设计。结果表明,采用聚醚型聚氨酯橡胶UR101为主体材料,加入20份炭黑N220或气相法白炭黑,添加适当的硅烷偶联剂、防老剂和碳纳米管等,可得到综合性能良好的硫化胶,其DIN磨耗量可低至30~40 mm^3。  相似文献   

11.
研究了DCP用量对EPDM力学性能、老化性能的影响。结果表明,采用过氧化物DCP硫化体系的力学性能优于硫磺硫化体系。DCP硫化的EPDM加入抗氧剂MB后具有较高的耐热氧老化性能,显示出MB具有较高的防护效能。  相似文献   

12.
采用硫化特性参数、溶胀指数和DSC谱图等表征了聚氨酯橡胶(PUR)/氯丁橡胶(CR)共混胶的共硫化性能,并研究了PUR/CR的共混比、补强体系与软化体系等对共混胶的硫化特性的影响.结果表明,采用过氧化二异丙苯/氧化镁(DCP/MgO)复合硫化体系,可以使PUR/CR共混胶达到共硫化;增加PUR和炭黑的用量,减少软化剂的用量,则共混胶料的转矩增大;增加PUR用量,可以加快共混胶料的硫化速度,其它因素对硫化速度的影响不明显.当PUR/CR共混比为20/80、DCP 3份、MgO 4份、炭黑N550 30份、软化剂聚异丁烯(PIB)5份时,共混硫化胶有较好的综合性能.  相似文献   

13.
改性蓖麻油基软质聚氨酯泡沫塑料的研究   总被引:1,自引:0,他引:1  
本文研究了环氧蓖麻油配比和环氧值对蓖麻油基软质聚氨酯泡沫物理性能的影响规律,并对原料配方进行了优化,制得了适宜不同需要的改性蓖麻油基软质泡沫,使蓖麻油基软质泡沫的手感、耐老化性能明显改善。  相似文献   

14.
The present article focuses on changes in the mechanical properties of an all-oxide fiber-reinforced composite following long-term exposure (1000 h) at temperatures of 1000–1200°C in air. The composite of interest derives its damage tolerance from a highly porous matrix, precluding the need for an interphase at the fiber–matrix boundary. The key issue involves the stability of the porosity against densification and the associated implications for long-term durability of the composite at elevated temperatures. For this purpose, comparisons are made in the tensile properties and fracture characteristics of a 2D woven fiber composite both along the fiber direction and at 45° to the fiber axes before and after the aging treatments. Additionally, changes in the state of the matrix are probed through measurements of matrix hardness by Vickers indentation and through the determination of the matrix Young's modulus, using the measured composite moduli coupled with classical laminate theory. The study reveals that, despite evidence of some strengthening of the matrix and the fiber–matrix interfaces during aging, the key tensile properties in the 0°/90° orientation, including strength and failure strain, are unchanged. This strengthening is manifested to a more significant extent in the composite properties in the ±45° orientation, wherein the modulus and the tensile strength each exhibit a twofold increase after the 1200°C aging treatment. It also results in a change in the failure mechanism, from one involving predominantly matrix damage and interply delamination to one which is dominated by fiber fracture. Additionally, salient changes in the mechanical response beyond the maximum load suggest the existence of an optimum matrix strength at which the fracture energy in the ±45° orientation attains a maximum. The implications for long-term durability of this class of composite are discussed.  相似文献   

15.
井玉  吴明生 《橡胶工业》2019,66(6):0440-0444
采用凝固剂浸渍法制备天然胶乳硫化胶膜,并对其结构和性能进行研究。结果表明:天然胶乳预硫化程度随硫黄用量的增加而增大;胶膜硫化后的交联程度随硫黄用量的增加先增大后减小,在硫黄用量为1.25份时达到最大值;拉伸强度随硫黄用量的增加先增大后减小,在硫黄用量为1份时达到最大值,而拉断伸长率呈下降趋势;当硫黄用量为1份时达到最佳致密性。  相似文献   

16.
室温固化高强度聚醚型聚氨酯弹性体的研制   总被引:12,自引:0,他引:12  
翟文  陈强  李玉莲 《弹性体》2003,13(3):11-13
介绍了室温固化高强度聚氨酯弹性体的合成方法及其性能。探讨了多元醇、异氰酸、稀释剂、交联剂等组份对聚氨脂弹性体性能的影响。试验证明聚醚型聚氨酯弹性体的硬度、拉伸强度和撕裂强度均随聚醚分子量的升高而下降,确定了本研究所需聚醚分子量为l000,采用PTMG:PPG=75:25(质量比)的混合多元醇合成的预聚体,并添加适量的稀释剂,在保证良好的物理性质和耐水解性能的前提下,降低了粘度,延长了釜中寿命,改善了施工工艺,降低了材料成本;采用混合胺固化剂降低了固化温度。该弹性体硬度高、强度高、回弹性好、耐磨、耐水解.并且满足了现场施工的要求.  相似文献   

17.
In this paper, a new approach to the paint composition design of WB 2-pack PUR coatings for car refinish application is presented. New hydroxy-functional binder emulsions are described that offer a better basis for the mixing process and the pot-life/reactivity balance with polyisocyanate hardeners. In addition, it will be shown that with these binder systems the overall balance of appearance, pot-life and curing speed can be enhanced to a very attractive level by the use of a well tuned catalyst package, allowing sufficient time for application, flow and de-aeration while offering the required fast curing characteristics as well. Thirdly, it will be shown how the aspects relating to undesired foam formation can be managed. Finally, the performance of low VOC paint compositions for car refinish application based on this new generation of WB 2-pack PUR system will be discussed.  相似文献   

18.
研究了NBR/HNBR共混比对其共混胶硫化特性、力学性能、耐热空气老化性能及耐臭氧性能的影响。结果表明,随着HNBR用量的增大,共混胶硫化时间先缩短后延长,力学性能先降低后升高,耐热空气老化性能提高,耐臭氧老化性能也提高。  相似文献   

19.
分别研究了预分散酚醛树脂HY-2045(预)、HY-2055(预)和SP-1055(预)对CIIR胶料硫化特性、力学性能及100℃×72h热空气老化性能的影响,并与原树脂HY-2045(原)、HY-2055(原)和SP-1055(原)的影响效果进行了对比。结果表明,与原酚醛树脂相比,预分散酚醛树脂在CIIR橡胶中的分散性、硫化胶拉伸强度和拉断伸长率均获得提高。加入SP-1055(预)可明显缩短CIIR胶料的t90;加入HY-2045(预)可使胶料的t10和t90延长,交联密度、硬度、100%定伸应力和拉伸强度均最小,拉断伸长率最大;加入HY-2055(预)可使胶料的t90延长,其他性能与加入SP-1055(预)的胶料相差不大。加入HY-2055(预)的硫化胶100℃×72h热空气老化后性能变化最小。  相似文献   

20.
以聚氨酯制品为例,介绍了制品快速加工的实验过程,并对制品的尺寸精度。加工时间和加工成本等进行了分析。基本步骤为:首先使用立体光固化快速成型设备制造制品的原型,再以原型为基础模型快速制造模具,然后使用反应注射成型设备快速加工制品,结果表明,使用快速加工技术,聚氨酯制品加工周期约为30h,总体加工成本低,制品尺寸精度符合设计要求。  相似文献   

设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号