本文采用直流反应磁控溅射法及能量过滤磁控溅射技术,以玻璃为衬底制备了纳米TiO2薄膜和纳米TiO2/ITO复合薄膜.利用X射线衍射(XRD) 、扫描电镜(SEM) 、紫外-可见分光光度计(UV-VIS) 、椭偏光谱仪(VASE型)和接触角测定等手段对薄膜进行了表征.研究表明:纳米TiO2/ITO复合薄膜表面水的初始接触角较纳米TiO2薄膜明显减小,ITO膜层的存在抑制了光生载流子的复合,在紫外光照射5min后接触角迅速下降,紫外光照射30min后接近0°,亲水性较纳米TiO2薄膜有明显提高;应用能量过滤磁控溅射技术制备的薄膜晶粒尺寸减小至10nm左右,薄膜表面平整,吸收边波长"蓝移"至320nm;纳米TiO2/ITO复合薄膜在可见光波段的透过率下降至60%左右,较纳米TiO2薄膜的80%明显降低. 相似文献
2.
3.
《功能材料》2016,(12)
采用直流磁控溅射法在不同溅射功率和工作气压条件下沉积Cu薄膜,对其进行X射线衍射、原子力显微镜、电阻率测试,分析了工艺参数对Cu薄膜的沉积速率、微观结构和电阻率的影响。通过紫外光刻技术将Cu薄膜制成桥箔,采用电爆测试平台获得Cu桥箔的电爆参数,研究了Cu薄膜的晶粒尺寸、择优取向对其电爆性能的影响。结果表明:随溅射功率的增大,Cu薄膜的沉积速率增加、晶粒尺寸增大、Cu(111)晶面择优取向特性变差,且电阻率降低;随溅射工作气压增大,Cu薄膜的沉积速率降低、晶粒尺寸减小、Cu(111)晶面择优取向越明显,且电阻率增加。对于相同桥区参数的Cu桥箔,晶粒尺寸越小,其爆发时刻就越早;Cu(111)晶面择优取向越明显,其爆发电流和峰值功率就会越大。 相似文献
4.
5.
6.
退火温度对纳米TiO2薄膜结构和亲水性的影响 总被引:7,自引:1,他引:7
采用射频磁控溅射方法制备出纳米二氧化钛(TiO2)薄膜,研究了不同退火温度对薄膜微观结构和超亲水性的影响.结果表明:退火温度升高,晶粒长大,孔隙率减小;常温制备300 ℃以下退火的TiO2薄膜为无定形结构,亲水性差;400 ℃~650 ℃退火的薄膜为锐钛矿结构,表现出超亲水性;800 ℃退火薄膜为金红石结构,亲水性有所下降. 相似文献
7.
8.
溅射功率对TiO2薄膜结构与特性的影响 总被引:2,自引:1,他引:2
采用射频磁控溅射法,在室温和不同功率条件下,在soda-lime玻璃衬底上成功制备出TiO2薄膜。运用X射线衍射(XRD)仪、能谱仪、拉曼(Raman)光谱仪、PL光谱、紫外—可见(UV-VIS)分光光度计等对样品进行了表征分析。分析结果表明:当溅射功率小于100 W时,在soda-lime玻璃衬底上制备的TiO2薄膜为无定形结构。当溅射功率大于等于150 W时,所得TiO2薄膜中出现锐钛矿结构。在本实验中,随溅射功率的增加,TiO2薄膜的结晶越好,晶粒的粒径不断增大且沿(101)取向生长。当在氧气气氛中500℃退火2 h后,制备的TiO2薄膜中锐钛矿相晶粒尺寸增加了17%。在本实验条件下,随着溅射功率的增加,薄膜厚度明显增加,薄膜厚度与溅射功率基本成线性关系。通过光催化降解实验得出,所得到的纳米TiO2薄膜对亚甲基兰溶液具有较强的降解能力。 相似文献
9.
纳米钛基TiO_2薄膜生长特点和生物活性研究 总被引:2,自引:0,他引:2
采用直流磁控溅射法分别在纳米晶体钛和粗晶粒工业纯钛表面沉积TiO2薄膜,研究了纳米钛基TiO2薄膜的结构形貌、形核、生长、晶体结构和体外生物活性。用扫描电镜和X射线衍射仪分析了薄膜的表面形貌和晶体结构,用体外模拟人体体液浸泡诱导羟基磷灰石生长实验表征薄膜的生物活性。结果表明:纳米钛基薄膜形核率高,薄膜非常致密、光滑,晶粒细小,仅为粗晶粒钛基TiO2薄膜晶粒尺寸的一半,约100nm;钛基材纳米晶体化可促进薄膜由锐钛矿相向金红石相转变;钛基材纳米化可显著提高自身及其表面TiO2薄膜的生物活性。 相似文献
10.
退火温度对TiO2薄膜结构和表面形貌的影响 总被引:3,自引:0,他引:3
研究了退火温度对中频交流反应磁控溅射技术制备的TiO2 薄膜结构和表面形貌的影响。利用X射线衍射仪和原子力显微镜 ,检测了TiO2 薄膜的晶体结构和表面形貌。实验结果显示 :沉积态TiO2 薄膜为非晶态 ;低温 (70 0℃以下 )退火后 ,TiO2 薄膜出现锐钛矿相 ,晶粒长大不明显 ;高温退火 (90 0℃以上 )后 ,薄膜转变为金红石相 ,晶粒由柱状转变为棱状 ,并迅速长大至微米量级 相似文献
11.
A method is proposed for estimating the parameters of a mixture of exponential and Weibull distributions for which the accuracy of preliminary estimates obtained by graphical analysis is refined in accordance with the criterion of maximum likelihood. The efficiency of the proposed method is supported by the results of statistical modeling. 相似文献
12.
An approximate analytical expression is derived for the velocity of the front of the wave of change of boiling modes on a
rod and on a plate. The impact of the Thomson effect and of the heater orientation in the gravity field is included. Adequate
agreement is demonstrated between the derived relations and experimental data. 相似文献
13.
Liebert A Wabnitz H Grosenick D Möller M Macdonald R Rinneberg H 《Applied optics》2003,42(28):5785-5792
A novel method for the determination of the optical properties of tissue from time-domain measurements is presented. The data analysis is based on the evaluation of the first moment and the second centralized moment, i.e., the mean time of flight and the variance of the measured distribution of times of flight (DTOF) of photons injected by short (picosecond) laser pulses. Analytical expressions are derived for calculation of absorption and of reduced scattering coefficients from these moments by application of diffusion theory for infinite and semi-infinite homogeneous media. The proposed method was tested on experimental data obtained with phantoms, and results for absorption and reduced scattering coefficients obtained by the proposed method are compared with those obtained by fitting of the same data with analytical solutions of the diffusion equation. Furthermore, the accuracy of the moment analysis was investigated for a range of integration limits of the DTOF. The moment analysis may serve as a comparatively fast method for evaluating optical properties with sufficient accuracy and can be used, e.g., for on-line monitoring of optical properties of biological tissue. 相似文献
14.
15.
16.
水三相点是开尔文热力学温度的唯一基准点,也是ITS-90国际温标重要的定义固定点。因此,水三相点不确定度分析对整个温标的建立、温度量值传递起着至关重要的作用。近3年来,中国计量科学研究院研制出一系列高质量的水三相点容器,加强了水三相点的研究,为不确定度的分析提供了更为可靠的实验依据。同时,不确定度的分析也是客观评价新研制容器性能的一个重要指标。因此,根据实验结果对新研制容器所复现的水三相点进行了不确定度评定。评定结果表明,其扩展不确定度为0.16mK(k=2.69,P=0.99)。 相似文献
17.
18.
19.