A series of polystyrene‐b‐poly(dimethylsiloxane)‐b‐polystyrene (PS/PDMS/PS) triblock copolymers had been synthesized by atom transfer radical polymerization (ATRP). The products had been characterized by Fourier transform infrared, gel permeation chromatography, differential scanning calorimetry, thermogravimetric analysis, contact angle, and scanning electron microscope. The results indicate that the PS chains have been successfully blocked onto the PDMS back bone, and the PS‐b‐PDMS‐b‐PS triblock copolymers have low‐surface tension, good thermal stability, and microphase separation configuration. © 2012 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013  相似文献   

2.
This study presented the investigations on the synthesis of a novel biodegradable block copolymer of pluronic‐b‐poly(L ‐lysine) (pluronic‐b‐PLL), which combined the characteristics of aliphatic polyester and poly(amino acids). The synthesis work started with end‐capping of pluronic with Nt‐butoxycarbonyl‐L ‐phenylalanine using dicyclohexylcarbodiimide in the presence of 4‐dimethylaminopyridine, followed by a deprotection process to obtain the amino‐terminated pluronic; the new primary amino group in the modified pluronic initiated ring‐opening polymerization of amino acid N‐carboxyanhydride, which afforded the pluronic‐b‐poly(Nε‐(Z)‐L ‐lysine) block copolymer. Finally, removal of the side‐chain Nε‐(carbonybenzoxy) end protecting groups yields the block copolymer of pluronic‐b‐PLL. The products were characterized by 1H‐NMR, FTIR, DSC, and GPC. The block copolymer micelle containing the anticancer drug paclitaxel was prepared by the double emulsion method. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009  相似文献   

3.
The synthesis of diblock copolymers using atom transfer radical polymerization, ATRP, of n‐butyl methacrylate, BMA, and methyl methacrylate, MMA, is reported. These copolymers were prepared from 2‐bromoisobutyryl‐terminated macroinitiators of poly(MMA) and poly(BMA), using copper chloride, CuCl,/N,N,N′,N″,N″‐pentamethyldiethylenetretramine, PMDETA, as the catalyst system, at 100°C in bulk and in benzonitrile solution. The block copolymers were characterized by means of size‐exclusion chromatography, SEC, and 1H‐NMR spectroscopy. The SEC analysis of the synthesized diblock copolymers confirmed important differences in the molecular weight control depending on the reaction medium (solvent effect) and the chemical structure of the macroinitiator used. In addition, differential scanning calorimetry, (DSC) measurements were performed, showing for all the copolymers a phase separation. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 84: 2683–2691, 2002  相似文献   

4.
A new nanoparticle/block copolymer (NP/BCP) hybrid material combining the unique properties of BCP poly(styrene)‐b‐poly(d ‐lactide) (PS‐b‐PDLA) and inorganic NP quantum dots CdSe was developed. A systematic study on the microphase separation of a series of PS‐b‐PDLAs by small‐angle X‐ray scattering showed that the degree of order of the separated microdomains depended on the initial state of the BCP and the measurement temperature and can be improved through isothermal crystallization of PDLA, thermal annealing and shear field etc. Incorporating a small amount of NPs into the BCP matrix can improve the mobility of the polymer chains and thus promote self‐assembly of the BCP, which leads to hierarchically ordered structures. Excess NPs, however, cannot be completely incorporated into the PDLA domains, resulting in the phase transformation of the BCP, destruction of the ordered structure and even macroscopic phase separation due to the aggregation of NPs. An important observation is that stereocomplexation between PDLA and poly(l ‐lactide) could provide a driving force to promote microphase separation of the BCP. The strategy presented in the current work has potential applications for developing highly ordered NP/BCP hybrid materials. © 2014 Society of Chemical Industry  相似文献   

5.
Polyester‐polyether segmented block copolymers of poly[(butylene succinate)‐co‐poly(butylene terephthalate)] (PBS–PBT) and poly(tetramethylene glycol) (PTMG) (Mn = 2000) with various compositions were synthesized. PBT content in the PBS was adjusted to ca. 5 mol %. Their thermal and mechanical properties were investigated. In the case of copolymer, the melting point of the PBS–PBT control was 107.8°C, and the melting point of the copolymer containing 70 wt % of PTMG was 70.1°C. Crystallinity of soft segment was 5 ∼ 17%, and that of hard segment was 42 ∼ 59%. The breaking stress of the PBS–PTMG control was 47 MPa but it decreased with increasing PTMG content. In the case of copolymer containing 70 wt % of PTMG, breaking stress was 36 MPa. Contrary to the decreasing breaking stress, breaking strain increased from 300% for PBS–PBT control to 900% for a copolymer containing 70 wt % of PTMG. The shape recovery ratios of the copolymer containing 70 wt % PTMG were almost twice of those of copolymers containing 40 wt % PTMG. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 79: 2067–2075, 2001  相似文献   

6.
Acrylic acid was crosslinked with N,N′‐methylenebisacrylamide and converted to bioactive hydrogels by neutralization with different amino containing compounds. Several amino containing compounds were used such as 2‐aminopyridine, triethanol amine, hexamethylenetetramine (HMTA), pyridine, and imidazole. The best crosslinker ratio was determined in addition to the maximum absorbed water in different mediums. The antibacterial activity of the prepared gels were examined against examples of Gram‐positive (Staphylococcus aureus) and Gram‐negative bacteria (Escherichia coli) using agar plate method. The study was extended by evaluating one of prepared gels in columns as models for water filters. All prepared gels showed antibacterial action in agar plate method against both bacterium and the column method using one of the prepared gels showed excellent filtration and biocidal action. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

7.
Polystyrene‐b‐poly(dimethylsiloxane)‐b‐polystyrene (Pst‐b‐PDMS‐b‐PSt) triblock copolymers were synthesized by atom transfer radical polymerization (ATRP). Commercially available difunctional PDMS containing vinylsilyl terminal species was reacted with hydrogen bromide, resulting in the PDMS macroinitiators for the ATRP of styrene (St). The latter procedure was carried out at 130°C in a phenyl ether solution with CuCl and 4, 4′‐di (5‐nonyl)‐2,2′‐bipyridine (dNbpy) as the catalyzing system. By using this technique, triblock copolymers consisting of a PDMS center block and polystyrene terminal blocks were synthesized. The polymerization was controllable; ATRP of St from those macroinitiators showed linear increases in Mn with conversion. The block copolymers were characterized with IR and 1H‐NMR. The effects of molecular weight of macroinitiators, macroinitiator concentration, catalyst concentration, and temperature on the polymerization were also investigated. Thermodynamic data and activation parameters for the ATRP are reported. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 92: 3764–3770, 2004  相似文献   

8.
Poly(butyl methylacrylate)–b–poly(dimethylsiloxane)–b–poly(butyl methylacrylate) (PBMA–b–PDMS–b–PBMA) triblock copolymers were synthesized by atom transfer radical polymerization (ATRP). The reaction of α,ω‐dichloride PDMS with 2′‐hydroxyethyl‐2‐bromo‐2‐methylpropanoate gave suitable macroinitiators for the ATRP of BMA. The latter procedure was carried out at 110°C in a phenyl ether solution with CuCl and 4,4′‐di (5‐nonyl)‐2,2′‐bipyridine (dNbpy) as the catalyzing system. The polymerization was controllable, with the increase of the monomer conversion, there was a nearly linear increase of molecular weight and a decrease of polydispersity in the process of the polymerization, and the rate of the polymerization was first‐order with respect to monomer conversion. The block copolymers were characterized with IR and 1H‐NMR and differential scanning calorimetry. The effects of macroinitiator concentration, catalyst concentration, and temperature on the polymerization were also investigated. Thermodynamic data and activation parameters for the ATRP were reported. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 92: 532–538, 2004  相似文献   

9.
Polyamide‐6 (PA6)/polybutadiene (PB) block copolymers were synthesized with macroactivators (MAs) based on hydroxyl‐terminated polybutadiene functionalized with diisocyanates and having three N‐acyllactam chain‐growing centers per molecule. Two different diisocyanates, hexamethylene diisocyanate and isophorone diisocyanate, were applied as precursors for the MAs. The sodium salt of ε‐caprolactam was chosen as an initiator. The influence of the MA type and concentration on the anionic ring‐opening polymerization of ε‐caprolactam at 180°C was studied. A large percentage of the gel fraction in the copolymers was estimated, indicating crosslinked macromolecules. The structure and phase behavior of the copolymers were investigated with differential scanning calorimetry, wide‐angle X‐ray scattering, thermogravimetric analysis, and dynamic mechanical thermal analysis. In the copolymers, only the PA6 chains crystallized, and the crystallinity depended on the PB content. Different glass‐transition temperatures for the PB blocks and PA6 blocks were observed, indicating microphase separation in the copolymers. The mechanical properties of the copolymers were studied by notched impact testing and hardness measurements. The impact strength increased linearly with the soft component concentration up to 10 wt % and reached values six times higher than those of the PA6 homopolymer. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 89: 711–717, 2003  相似文献   

10.
A series of new amphiphilic poly[methyl(3,3,3‐trifluoropropyl) siloxane]‐b‐poly(ethyleneoxide) (PMTFPS‐b‐PEO) diblock copolymers with different ratio of hydrophobic segment to hydrophilic segment were prepared by coupling reactions of end‐functional PMTFPS and PEO homopolymers. PMTFPS‐b‐PEO diblock copolymers synthesized were shown to be well defined and narrow molecular weight distributed by characterizations such as NMR, GPC, and FTIR. Additionally, the solution properties of these diblock copolymers were investigated using tensiometry and transmission electron microscopy. Interestingly, the critical micellization concentration increases with increasing length of hydrophobic chain. Transmission electron microscopy studies showed that PMTFPS‐b‐PEO diblock copolymers in water preferentially aggregated into vesicles. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012  相似文献   

11.
The synthesis of triblock copolymer poly(octadecyl acrylate‐b‐styrene‐b‐octadecyl acrylate), using atom transfer radical polymerization (ATRP), is reported. The copolymers were prepared in two steps. First, polystyrene was synthesized by ATRP using α,α′‐dichloro‐p‐xylene/CuBr/bpy as the initiating system; Second, polystyrene was further used as macroinitiator for the ATRP of octadecyl acrylate to prepare ABA triblock copolymers in the presence of FeCl2·4H2O/PPh3 in toluene. Polymers with controlled molecular weight (Mn = 17,000–23,400) and low polydispersity index value (1.33–1.44) were obtained. The relationship between molecular weight versus conversion showed a straight line. The effect of reaction temperature on polymerization was also investigated, showing a faster polymerization rate under higher temperature. The copolymers were characterized by FTIR, 1H‐NMR, DSC, and GPC and the crystallization behavior of the copolymers was also studied. © 2004 Wiley Periodicals, Inc. J Appl Polym Sci 93: 1539–1545, 2004  相似文献   

12.
Well‐defined poly(dimethylsiloxane)‐block‐poly(methyl methacrylate)‐block‐poly(2,2,3,3,4,4,4‐heptafluorobutyl methacrylate) (PDMS‐b‐PMMA‐b‐PHFBMA) triblock copolymers were synthesized via atom transfer radical polymerization (ATRP). Surface microphase separation in the PDMS‐b‐PMMA‐b‐PHFBMA triblock copolymer films was investigated. The microstructure of the block copolymers was investigated by transmission electron microscopy (TEM) and atomic force microscopy (AFM). Surface composition was studied by X‐ray photoelectron spectroscopy (XPS). The chemical composition at the surface was determined by the surface microphase separation in the PDMS‐b‐PMMA‐b‐PHFBMA triblock copolymer films. The increase of the PHFBMA content could strengthen the microphase separation behavior in the PDMS‐b‐PMMA‐b‐PHFBMA triblock copolymer films and reduce their surface tension. Comparison between the PDMS‐b‐PMMA‐b‐PHFBMA triblock copolymers and the PDMS‐b‐PHFBMA diblock copolymers showed that the introduction of the PMMA segments promote the fluorine segregation onto the surface and decrease the fluorine content in the copolymers with low surface energy. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

13.
Poly(n‐butyl methacrylate)‐b‐polystyrene‐b‐poly(n‐butyl methacrylate) (PBMA‐b‐PSt‐b‐PBMA) triblock copolymers were successfully synthesized by emulsion atom transfer radical polymerization (ATRP). Difunctional polystyrene (PSt) macroinitiators that contained alkyl chloride end‐groups were prepared by ATRP of styrene (St) with CCl4 as initiator and were used to initiate the ATRP of butyl methacrylate (BMA). The latter procedure was carried out at 85°C with CuCl/4,4′‐di (5‐nonyl)‐2,2′‐bipyridine (dNbpy) as catalyst and polyoxyethylene (23) lauryl ether (Brij35) as surfactant. Using this technique, triblock copolymers consisting of a PSt center block and PBMA terminal blocks were synthesized. The polymerization was nearly controlled, ATRP of St from those macroinitiators showed linear increases in the number average molecular weight (Mn) with conversion. The block copolymers were characterized with infrared (IR) spectroscopy, hydrogen‐1 nuclear magnetic resonance (1HNMR), and differential scanning calorimetry (DSC). The effects of the molecular weight of macroinitiators, concentration of macroinitiator, catalyst, emulsion, and temperature on the polymerization were also investigated. Thermodynamic data and activation parameters for the ATRP were also reported. POLYM. ENG. SCI., 45:1508–1514, 2005. © 2005 Society of Plastics Engineers  相似文献   

14.
A saturated star‐shaped polystyrene‐b‐poly(ethylene‐co‐propylene) block copolymer, (SEP)star, was synthesized for use as a viscosity index improver in lubricants. Polystyrene‐b‐polyisoprene arms were first made anionically, followed by a linking reaction at the optimum temperature of 60°C with divinylbenzene. The resulting star‐shaped (SI)star was hydrogenated to eliminate the double bonds on the polyisoprene segment, thus forming the star‐shaped (SEP)star. The number of arms on each molecule increased with an increase in the mol ratio of divinylbenzene to n‐butyllithium. Increasing the arm length adversely affected the linking efficiency but caused a slight increase in the degree of branching. The Tg of the poly(ethylene‐co‐propylene) block was 13°C higher than that of the original polyisoprene block. Compared with (SI)star, (SEP)star has a thermal decomposition temperature 50°C higher but independent of the arm length or the degree of branching. Viscosity measurements for (SEP)star revealed that intrinsic viscosity depends only on the arm length, but not on the degree of branching. Adding 1 wt % of (SEP)star markedly increased the viscosity index of a HN base oil. With a fixed arm length, a (SEP)star having a higher degree of branching increased the viscosity index more than that having a lower degree of branching. On the other hand, the viscosity index increased with an increase in the arm length when the degree of branching was fixed. The addition of 1wt % of (SEP)star increased the vioscosity index up to a number between 111 and 166, with the exact number depending upon its arm length and degree of branching. © 2001 John Wiley & Sons, Inc. J Appl Polym Sci 79: 1838–1846, 2001  相似文献   

15.
Advance polyamide‐6‐b‐polydimethylsiloxane (PA6‐b‐PDMS) multiblock copolymers were first synthesized via the polymerization in bulk. Binary carboxyl terminated PA6 was served as the hard segment and PDMS modified with hexamethylene diisocyanate (PDMS‐NCO) was the soft segment. A series of PA6‐b‐PDMS copolymers based on different content and length of soft segments were obtained. Interestingly, Differential scanning calorimetry (DSC) studies revealed no obvious change in melting temperature after introducing PDMS segments to copolymers. The high melting temperatures indicated these copolymers possess potential applications in automotive industry that require high continuous use temperatures. DSC and transmission electron microscopy studies both demonstrated increasing the length and the content of the soft segment contributed to increasing of the degree of microphase separation. However, the improvement of thermal stability resulting from PDMS segments was also observed by thermo gravimetric analysis. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2014 , 131, 41114.  相似文献   

16.
Polystyrene‐block‐poly(n‐butyl acrylate) block copolymers were prepared from 4‐oxo‐2,2,6,6‐tetramethylpiperidinooxy (4‐oxo‐TEMPO) capped polystyrene macroinitiators at a high temperature, 165°C. It was found that the number‐average molecular weight of PBA chains in block copolymers could reach above 10,000 rapidly at early stage of polymerization with a narrow polydispersity index of 1.2–1.4, but after that, the polymerization seemed to be retarded. Furthermore, according to the kinetic analysis, the concentration of 4‐oxo‐TEMPO was increased mainly by the hydrogen transfer reaction of hydroxylamine (4‐oxo‐TEMPOH) to growing radicals during polymerization. This increase in 4‐oxo‐TEMPO concentration could retard the growth of polymer chains. The rate constant of the hydrogen transfer reaction of 4‐oxo‐TEMPOH to growing radicals, kH, estimated by the kinetic model is about 9.33 × 104M‐1s?1 at 165°C. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009  相似文献   

17.
The copolymerization system of acrylamide (AM) and styrene (St) was acquired by using amphiphilic block copolymer PAM‐b‐PSt with lower molecular weight as polymeric surfactant, and then the microemulsion phase diagram was drawn. The appropriate copolymerization systems were chosen in the phase diagram, and higher molecular weight amphiphilic block copolymers PAM‐b‐PSt were prepared by self‐emulsifying microemulsion method. The chemical composition and structure of the products were analyzed by FTIR, 1H‐NMR, 13C‐NMR, GPC, and UV; the block structure of products was characterized by DSC, and the hydrophobic association property of the products was studied by the fluorescence probe and rotating viscosity measurement. The results showed that O/W microemulsion was also acquired by using the polymeric surfactant; 3 g polymeric surfactant was only used to disperse 0.25 g St into aqueous solution, which showed higher emulsifying efficiency. At the same time, the use of self‐emulsifying microemulsion copolymerizing system can avoid back treatment of small molecular surfactant and the purified block polymer was prepared in one step; the prepared copolymers have good hydrophobic association properties and their aqueous solution showed evident viscosity increment. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009  相似文献   

18.
In this article, a conductive foam based on a novel styrene‐based thermoplastic elastomer called poly(styrene‐b‐butadiene‐co‐styrene‐b‐styrene) tri‐block copolymer S(BS)S was prepared and introduced. S(BS)S was particularly designed for chemical foaming with uniform fine cells, which overcame the shortcomings of traditional poly(styrene‐b‐butadiene‐b‐styrene) tri‐block copolymer (SBS). The preparation of conductive foams filled by the carbon black was studied. After the detail investigation of cross‐linking and foaming behaviors using moving die rheometer, the optimal foaming temperature was determined at 180°C with a complex accelerator for foaming agent. Scanning electron microscopy (SEM) images shown that the cell bubbles of conductive foam were around 30–50 µm. The conductivity of foams was tested using a megger and a semiconductor performance tester. SEM images also indicated that the conductivity of foams was mainly affected by the distribution of carbon black in the cell walls. The formation of the network of the carbon black aggregates had a contribution to perfect conductive paths. It also found that the conductivity of foams declined obviously with the foaming agent content increasing. The more foaming agent led to a sharp increasing of the number of cells (from 2.93 × 106 to 6.20 × 107 cells/cm3) and a rapid thinning of the cell walls (from 45.3 to 1.4 µm), resulting in an effective conductive path of the carbon black no forming. The conductive soft foams with the density of 0.48–0.09 g/cm3 and the volume resistivity of 3.1 × 103?2.5 × 105 Ω cm can be easily prepared in this study. © 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015 , 132, 41644.  相似文献   

19.
A new regular ABA-type triblock copolymer has been synthesized by polycondensation of the acid chloride of carboxy-terminated butadience-acrylonitrile rubber (CTBN) with hydroxyterminated polyethylene isophthalate (PEI) oligomer. This block copolymer was characterized by elemental (nitrogen) analysis, vapor pressure osmometry, viscometry, and IR and NMR spectroscopy. Quantitative estimation of block segments has been carried out by measuring the area under peaks assigned to various protons in the NMR spectrum of the polymer. NMR spectral analysis has been found to agree well with the nitrogen analysis of the polymer. The solubility and solution viscosity behavior of the polymer has also been studied.  相似文献   

20.
Composites which combine biocompatible polymers and hydroxyapatite are unique materials with regards to their mechanical properties and bioactivity in the development of temporary bone‐fixation devices. Nanocomposites based on a biocompatible and amphiphilic triblock copolymer of poly(l‐ lactide) (PLLA) and poly(ethylene oxide) (PEO) —PLLA‐b‐PEO‐b‐PLLA— and neat (nHAp) or PEO‐modified (nHAp@PEO) hydroxyapatite nanoparticles were prepared by dispersion in benzene solutions, followed by freeze‐drying and injection moulding processes. The morphology of the copolymers of a PEO block dispersed throughout a PLLA matrix was not changed with addition of the nanofillers. The nHAp particles were spherical and, after modification, the nHAp@PEO nanoparticles were partially agglomerated. In the nanocomposites, these particles characteristics remained unchanged, and the nHAp particles and nHAp@PEO agglomerates were uniformly dispersed through the copolymer matrix. These particles acted as nucleating agents, with nHAp@PEO being more efficient. The incorporation of nHAp increased both the reduced elastic modulus (~22%) and the indentation hardness (~15%) in comparison to the copolymer matrix, as determined by nanoindentation tests, while nHAp@PEO addition resulted in lower increments of these mechanical parameters. The incorporation of untreated nHAp was, therefore, more beneficial with regards to the mechanical properties, since the amphiphilic PLLA‐b‐PEO‐b‐PLLA matrix was already efficient for nHAp nanoparticles dispersion. © 2016 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2016 , 133, 44187.  相似文献   