The polymerizations of norbornene were investigated using a series of bis(β‐ketoamino)nickel(II) complexes( 1–6 ) in combination with methylaluminoxane (MAO) in toluene solution. The effects of catalyst structure, Al/Ni molar ratio, reaction temperature, and reaction time on catalytic activity and molecular weight of the polynorbornene were examined in detail. The electronic effect of the substituent around the imino group in the ligand is stronger than the steric bulk one on the polymerization activities, and the activities are in the order of 1 > 2 > 4 > 5 > 6 > 3 . The obtained polynorbornenes were characterized by means of 1H‐NMR, 13C‐NMR, FTIR, TG, and WAXD techniques. The analyses results of polymers' structures and properties indicate that the polymerization reaction of norbornene runs in vinyl‐addition polymerization mode. The obtained polynorbornene was confirmed to be vinyl‐type and atactic polymers and showed good thermostability (Tdec > 458°C) and were noncrystalline but had short‐range order. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 4172–4180, 2006  相似文献   

2.
The copolymerization of styrene with ethylene was promoted by CpTiCl3/BDGE/Zn/MAO catalyst system combining free radical polymerization with coordination polymerization via sequential monomer addition strategy in one‐pot. The effect of polymerization conditions such as temperature, time, ethylene pressure, and Al/Ti molar ratio on the polymerization performance was investigated. The hydroxy‐functionalized aPS‐b‐random copolymer‐b‐PE triblock copolymer was obtained by solvent extraction and determined by GPC, DSC, WAXD, and 13C‐NMR. The DSC result indicated that the aPS‐b‐random copolymer‐b‐PE had a Tg at 87°C and a Tm at 119°C which attributed to the Tg of aPS segment and the Tm of PE segment, respectively. The microstructure of the hydroxy‐functionalized aPS‐b‐random copolymer‐b‐PE was further confirmed by WAXD, 13C‐NMR, and 1H‐NMR analysis; and these results demonstrated that the obtained block copolymer consisted of aPS segment, S‐E random copolymer segment, and crystalline PE segment. The connection polymerization of the hydroxy‐functionalized aPS with random copolymer‐b‐PE was revealed by GPC results. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

3.
A homologous series of aliphatic polycarbonates with different side‐chain lengths was synthesized by ring‐opening polymerization of terminal epoxides with CO2 using zinc adipionate as catalyst [patented process of Empower Materials (formerly PAC Polymers Inc.)]. Additionally, a polycarbonate was made having a cyclohexane unit in its backbone, together with a terpolymer having both cyclohexane and propylene units. After characterization of thermal properties the aliphatic polycarbonates were found to be completely amorphous. Polycarbonates derived from long‐chain epoxides showed a glass‐transition temperature (Tg) below room temperature, whereas polycarbonates derived from cyclohexene oxide showed a Tg of 105°C, the highest yet reported for this class of polymers. The initial decomposition temperature of the polymers in air and nitrogen atmospheres was found to be less than 300°C. The mechanical properties and the dynamic mechanical relaxation behavior of the polymers were also reported. The effect of the chemical structure on the physical properties of aliphatic polycarbonates was discussed. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 89: 1163–1176, 2003  相似文献   

4.
Ester or cyano substituted tetracyclo [4.4.0.12,5.17,10]dodec-3-enes (1) were synthesized and their metathesis ring-opening polymerization was examined. The tungsten-based ternary catalyst system polymerized them very well. The polymers showed high glass transition temperatures (Tg) and no evidence of crystallization (e.g., the Tg of the polymer derived from 8-methyl-8-methoxycarbonyl substituted monomer (1a) was 207°C, and colorless transparent films could be casted from the solution of the polymer). The stability of these high Tg polymers were too unstable, so practical thermal molding methods could not be applied to them. The hydrogenation of these polymers with a palladium catalyst decreased Tg and greatly increased thermal stability. The physical and thermal properties of the hydrogenated polymers were thoroughly investigated. Monomer 1 was successfully copolymerized with other cyclic olefins. The resultant copolymers were hydrogenated, giving thermally stable polymers. In all cases examined in this study, a decrease of Tg by hydrogenation was about 35°C, regardless of the monomer structure. These results indicate that the main-chain mobility is the major contribution to the decrease of Tg. © 1997 John Wiley & Sons, Inc. J Appl Polym Sci 66: 367–375, 1997  相似文献   

5.
Poly(ethylene oxide)‐block‐poly(methacryl‐d ‐glucopyranoside) (PEO‐GP) and poly(methacryl‐d ‐glucopyranoside) (H‐GP) glycopolymers were synthesized by deacetylation of acetylated polymers which were synthesized via atom transfer radical polymerization. The synthesized glycopolymers were characterized using 1H NMR, 13C NMR and Fourier transform infrared (FTIR) spectroscopies, gel permeation chromatography (GPC), thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC). The deacetylated polymers exhibited onset decomposition temperatures about 60 °C lower compared to the polymers having acetyl pendants. The glass transition temperature (Tg) of the acetylated homopolymer was 133 °C and that of the PEO‐based block copolymer was 124 °C. The deacetylated polymers H‐GP and PEO‐GP exhibited Tg values of about ?30 °C. Biocompatibility of the H‐GP and PEO‐GP glycopolymers was obtained by studying osteoblast cell adhesion, viability and proliferation in vitro. The cell viability showed an increase with increasing concentration of H‐GP from 0.1 to 1 µmol L?1 and then decreased with further increase in its concentration (10–1000 µmol L?1). PEO‐GP did not show a significant variation in cell viability on variation of its concentration from 0.1 to 1000 µmol L?1. The significant improvement in biocompatibility with osteoblast cells in the presence of PEO‐GP was considered as due to the covalently bonded PEO segment of the methacrylate glycopolymer block. © 2014 Society of Chemical Industry  相似文献   

6.
Mixed‐substituent fluoroalkoxyphosphazene polymers bearing ~15% 1H,1H,2H,2H‐perfluorooctan‐1‐oxy or 1H,1H,2H,2H‐perfluorodecan‐1‐oxy side groups together with trifluoroethoxy cosubstituent groups were synthesized. The low reactivity of the long‐chain fluoroalkoxides and their limited solubility in organic solvents prevented higher levels of substitution. Moreover, the sodium alkoxides with two methylene residues adjacent to the oxygen proved to be unstable in solution due to elimination of NaF and precipitation of side products, and this limited the time available for chlorine replacement reactions. The resulting cosubstituent polymers were characterized by proton nuclear magnetic resonance (1H‐NMR), 31P‐NMR, 19F‐NMR, gel‐permeation chromatography, and differential scanning calorimetry. Unlike homo‐ or mixed‐substituent fluoroalkoxyphosphazene polymers, such as [NP(OCH2CF3)2]n (a microcrystalline thermoplastic, Tg ~ ?63°C, Tm ~ 242°C) or [NP(OCH2CF3)(OCH2(CF2)xCF2H)]n (PN‐F, a rubbery elastomer, Tg ~ ?60°C, but no detectable Tm), the new polymers are gums (Tg ~ ?50°C, but no detectable Tm) with molecular weights in the 105 g/mol rather than the 106 g/mol range. POLYM. ENG. SCI., 54:1827–1832, 2014. © 2013 Society of Plastics Engineers  相似文献   

7.
In this work, ethylene polymerization was investigated by using homogeneous and heterogenouse nickel α-diimine catalysts [1,4-bis(2,6-diisopropylphenyl) acenaphthene diimine nickel(II) dibromide]. Methyl aluminoxane (MAO) and triethyl aluminum (TEA) were used as cocatalysts in homogenous and heterogeneous polymerizations, respectively. The heterogeneous catalyst showed lower activity than its homogeneous equivalent. The influence of polymerization temperature and heterogenization conditions was studied on the microstructure properties of the prepared polymers. Increasing polymerization temperature (T P) up to 50 °C decreased the activity of both homogenous (LN) and heterogeneous (LNS) nickel α-diimine catalysts. The highest activities were 1286 and 982 kg PE (mol Ni bar h)?1 obtained at T P = 30 °C for LN and LNS catalysts, respectively. The polymer samples obtained by supported catalyst (LNS) showed lower unsaturation contents. Moreover, DSC analysis did not show any melting peaks for polymers obtained by LN catalyst due to their amorphous structure, which was confirmed by XRD analysis. The microstructure of the prepared polymers was completed by successive self-nucleation annealing (SSA) and was investigated by 13C NMR studies. The SSA thermogram of samples made by LNS catalyst exhibited several crystal types with different lamella thicknesses. The branches in polyethylene samples produced by homogenous catalyst were higher and showed more diversity. The total methyl branch percentages for both LN and LNS catalysts were 13.1 and 3.4%, respectively.  相似文献   

8.
BACKGROUND: This investigation evaluates the effectiveness of initiator adducts for living and controlled polymerization of methacrylates, crosslinking of dimethacrylates and thermal stabilities of the resulting polymers. Adducts of 2,2,6,6‐tetramethyl‐1‐piperidinyloxy with benzoyl peroxide and with azobisisobutyronitrile were prepared and evaluated as stabilized unimolecular initiators for the free radical polymerization of methacrylate monomers using sulfuric acid as catalyst. The monomers used were methyl methacrylate, triethylene glycol dimethacrylate (TEGDMA) and ethoxylated bisphenol A dimethacrylate (EBPADMA). RESULTS: Successful polymerization was achieved at 70 and 130 °C with reaction times ranging from 45 min to 120 h. The dispersity (D) of poly(methyl methacrylate) (PMMA) was 1.09–1.28. The livingness and extent of control over polymerization were confirmed with plots of Mn evolution as a function of monomer conversion and of the first‐order kinetics. The glass transition temperature (Tg) for PMMA was 123–128 °C. The degradation temperature (Td) for PMMA was 350–410 °C. Td for poly(TEGMA) was 250–310 °C and for poly(EBPADMA) was 320–390 °C. CONCLUSION: The initiators are suitable for free radical living and controlled polymerization of methacrylates and dimethacrylates under mild thermal and acid‐catalyzed conditions, yielding medium to high molecular weight polymers with low dispersity, high crosslinking and good thermal stability. Copyright © 2008 Society of Chemical Industry  相似文献   

9.
Four cyclotriphosphazene‐based benzoxazine monomers (I, II, III, and IV) with relatively high molecular weight were synthesized by a nucleophilic substitution reaction, and their chemical structures were confirmed by 1H‐NMR and 31P‐NMR. A new term, oxazine value (OV, similar to epoxy value), was first proposed to explain the structure–property relationship of the cured polymers. The polymerization behaviors of the four monomers were studied by differential scanning calorimetry and Fourier transform infrared spectroscopy. The maximum exothermic peaks of the four monomers are in the range 244–248 °C. All monomers possess a wide processing window despite their high molecular weight. The thermal stability, glass‐transition temperature (Tg), and mechanical properties of each cured polymer were studied by thermogravimetric analysis and dynamic mechanical thermal analysis. The char yield at 850 °C, Tg, and storage moduli of PIV (polybenzoxazine obtained from monomer IV) are 60.0%, 218 °C, and 9.0 GPa, respectively. The surface property and humidity absorption character of the cured polybenzoxazines were also studied. © 2016 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2017 , 134, 44453.  相似文献   

10.
A series of copolyarylates of bisphenol A (BPA) with varying ratios of diphenyl terephthalate (DPT) and diphenyl isophthalate (DPI) were prepared by melt polymerization at a temperature ranging from 200 to 290°C under reduced pressure in the presence of tin octoate catalyst. Tin octoate catalyst has been extensively used for the preparation of biodegradable polymers namely, poly(lactic acid), poly(glycolic acid), and poly(lactide‐glycolide) copolyesters. However, there are no reports on the preparation of copolyesters by melt polymerization using tin octoate catalyst. The effect of tin octoate catalyst was studied on the preparation of BPA/DPT/DPI copolyarylates. The copolyarylates were characterized by infrared and 1H NMR spectroscopy, solution viscosity, thermogravimetric analysis, differential scanning calorimetry, and X‐ray diffraction. The solution viscosities of copolyarylates were varied from 0.43 to 0.56 dL/g and the glass transition temperature (Tg) of copolyarylates was varied from 155 to 222°C by varying the ratio of DPT and DPI. Most of the copolyarylates were found to be soluble in commonly used organic solvents and had film‐forming properties. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 70–77, 2006  相似文献   

11.
Two phosphonate‐containing bismaleimide (BMI) [(4,4′‐bismaleimidophenyl)phosphonate] monomers with different melting temperatures and similar curing temperatures were synthesized by reacting N‐hydroxyphenylmaleimide with two kinds of dichloride‐terminated phosphonic monomers. The BMI monomers synthesized were identified with 1H‐, 13C‐, and 31P‐nuclear magnetic resonance (NMR) spectroscopy and elemental analysis. The phosphonate‐containing BMI monomers react with a free‐radical initiator to prepare phosphonate‐containing BMI polymers and also with various aromatic diamines to prepare a series of polyaspartimides as reactive flame retardants. The polymerization degrees of polyaspartimides depend on the alkalinity and nucleophility of diamines as chain extenders. Differential scanning calorimetry (DSC) and thermogravimetry analysis (TGA) were used to study the thermal properties of the phosphonate‐containing BMI resins such as the melting temperature, curing temperature, glass transition temperature (Tg), and thermal resistance. All the phosphonate‐containing BMI resins, except the BMI polymers, have a Tg in the range of 210–256°C and show 5% weight loss temperatures (T5%) of 329–434 and 310–388°C in air and nitrogen atmospheres, respectively. The higher heat resistance of cured BMI resin relative to the BMI polymer is due to its higher crosslinking density. Since the recrosslinking reactions of BMI polymers and polyaspartimides occur more easily in an oxidation environment, their thermal stabilities in air are higher than are those in nitrogen gas. In addition, the thermal decomposition properties of polyaspartimides depend on the structures and compositions of both the diamine segments and the BMI segments. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 83: 1919–1933, 2002  相似文献   

12.
Imidazole, 2‐methylimidazole and benzimidazole‐blocked aromatic and aliphatic diisocyanates have been prepared and polymerized with pyromellitic dianhydride in the presence of a basic catalyst. The polymers are characterized with FTIR, 1H NMR and 13C NMR spectroscopy and GPC, DSC and TGA. The structure–property relationship of blocked diisocyanates are discussed in terms of molecular weight of the polyimides obtained. Considering the blocking agent, GPC results show that the benzimidazole blocked adduct yields higher molecular weight polymer than the 2‐methylimidazole‐blocked adduct which, in turn, yields higher molecular weight polymer than the imidazole‐blocked adduct. Considering the structure of the isocyanate, the molecular weight of polymer increases from isophorone diisocyanate to hexamethylene diisocyanate and to toluene diisocyanate (TDI). DSC traces of the polymers derived from TDI show glass transitions (Tg) in the temperature range 152–180 °C and the values increase from the polymer based on imidazole‐blocked TDI to 2‐methylimidazole‐blocked TDI and to benzimidazole‐blocked TDI. © 2000 Society of Chemical Industry  相似文献   

13.
Synthesis of cyclic biopolymers from renewable monomers remains a big challenge because of lack of efficient catalysts. The organocatalyst of N‐heterocyclic carbene (NHC), (+)‐1‐methyl‐3‐menthoxymethyl imidazol‐2‐ylidene, is used to prepare cyclic polylactones including poly(ε‐caprolactone) (poly(ε‐CL)), poly(δ‐valearolactone) (poly(δ‐VL)), and poly(ε‐caprolactone‐co‐δ‐valearolactone) (poly(ε‐CL‐co‐δ‐VL)) via zwitterionic ring opening polymerization. The NHC catalyst is founded a highly efficient organic catalyst for the polymerization. The resulting cyclic polymers show a melting temperature (Tm) in a range of 20–60°C, which is dramatically lower than the Tm of cyclic poly(lactide) (Tm = 120–150°C). The resulting copolymer, cyclic poly(ε‐CL‐co‐δ‐VL) owns high molecular weight comparing with corresponding linear poly(ε‐CL‐co‐δ‐VL) produced by other catalysts. The synthesized cyclic homo and copolymers were characterized by 1H‐, 13C‐NMR spectroscopy, gel permeation chromatography, differential scanning calorimetry–thermogravimetric analysis and matrix‐assisted laser desorption ionization‐time of flight mass spectrometry. © 2012 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013  相似文献   

14.
Hyperbranched poly(silyl ester)s were synthesized via the A2 + B4 route by the polycondensation reaction. The solid poly(silyl ester) was obtained by the reaction of di‐tert‐butyl adipate and 1,3‐tetramethyl‐1,3‐bis‐β(methyl‐dicholorosilyl)ethyl disiloxane. The oligomers with tert‐butyl terminal groups were obtained via the A2 + B2 route by the reaction of 1,5‐dichloro‐1,1,5,5‐tetramethyl‐3,3‐diphenyl‐trisi1oxane with excess amount of di‐tert‐butyl adipate. The viscous fluid and soft solid poly(silyl ester)s were obtained by the reaction of the oligomers as big monomers with 1,3‐tetramethyl‐1,3‐bis‐β(methyl‐dicholorosilyl)ethyl disiloxane. The polymers were characterized by 1H NMR, IR, and UV spectroscopies, differential scanning calorimetry (DSC), and thermogravimetric analysis (TGA). The 1H NMR and IR analysis proved the existence of the branched structures in the polymers. The glass transition temperatures (Tg's) of the viscous fluid and soft solid polymers were below room temperature. The Tg of the solid poly(silyl ester) was not found below room temperature but a temperature for the transition in the liquid crystalline phase was found at 42°C. Thermal decomposition of the soft solid and solid poly(silyl ester)s started at about 130°C and for the others it started at about 200°C. The obtained hyperbranched polymers did not decompose completely at 700°C. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 3430–3436, 2006  相似文献   

15.
The Ritter reaction of plant oil triglycerides (such as soybean and sunflower oil) with acrylonitrile was used to introduce acrylamide functionality on the triglyceride. Acrylonitrile and triglycerides were reacted in the presence of H2SO4, and acrylamide derivatives were obtained in yields of 45 and 50% for sunflower oil and soybean oil, respectively. Radical initiated copolymerization of the acrylamide derivatives of the triglycerides with styrene produced semirigid polymers. Characterization of new monomers and polymers was done by 1H‐NMR, 13C‐NMR, IR, and MS. The swelling behavior of the crosslinked network polymers was determined in different solvents. Glass transiton temperature (Tg) of the cured resin was also determined by differential scanning calorimeter to be 40°C for soybean based polymer and 30°C for sunflower‐based polymer. Homo‐ and copolymerization behavior of acrylamide derivatives of methyl oleate (MOA) and methyl 10‐undecenoate (MUA) were also investigated. The reactivity ratios of these monomers with respect to styrene were determined by the Fineman–Ross method using 1H‐NMR spectroscopic data. The reactivity ratios were rsty = 1.776; rmoa = 0512 for MOA, and rsty = 1.142; rmua = 0.507 for MUA, respectively. Photopolymerization behaviors of MOA and MUA were also investigated using the photoDSC technique and the rate of polymerization of MUA is higher than that of MOA under the same conditions. © 2005 Wiley Periodicals, Inc. J Appl Polym Sci 97: 2264–2272, 2005  相似文献   

16.
A series of novel aromatic diamines containing cycloaliphatic moieties was synthesized by the reaction of cycloalkanones like cyclohexanone and cycloheptanone with 2,6‐dimethylaniline. The tetrimide diacid was synthesized using the prepared diamine with 3,3′,4,4′‐benzophenonetetracarboxylic acid dianhydride/pyromellitic dianhydride and p‐aminobenzoic acid. The polymers were prepared by treating the tetrimide diacid with different aromatic diamines. The structures of the monomers and polymers were identified using elemental analysis and Fourier transform infrared, 1H NMR and 13C NMR spectroscopy. The polymers show excellent solubility. The polymers are amorphous and have high optical transparency. They also show good thermal stability and their Tg value is found to be in the range 268–305 °C. Copyright © 2007 Society of Chemical Industry  相似文献   

17.
A novel diamine monomer having pendant 4‐(quinolin‐8‐yloxy) aniline group was successfully synthesized via aromatic substitution reaction of 8‐quinolinol with p‐fluoronitrobenzene followed by Pd/C catalyzed hydrazine reduction, amidation reaction between 4‐(quinolin‐8‐yloxy) aniline and 3,5‐dinitrobenzoylcholoride followed by Pd/C catalyzed hydrazine reduction. The diamine monomer was fully characterized by using FTIR, 1H‐NMR, 13C‐NMR, and elemental analysis. The diamine monomer was polymerized with various aromatic and aliphatic dicarboxylic acids to obtain the corresponding polyamides. The polyamides had inherent viscosity in the range of 0.30–0.41 dL/g and exhibited excellent solubility in the polar aprotic solvents such as DMAc, NMP, N,N‐dimethylformamide, Pyridine, and DMSO. The glass transition temperatures (Tg) of the polymers are high (up to 313°C) and the decomposition temperatures (Ti) range between 200 and 370°C, depending on the diacids residue in the polymers backbone. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2010  相似文献   

18.
Two oxetane‐derived monomers 3‐(2‐cyanoethoxy)methyl‐ and 3‐(methoxy(triethylenoxy)) methyl‐3′‐methyloxetane were prepared from the reaction of 3‐methyl‐3′‐hydroxymethyloxetane with acrylonitrile and triethylene glycol monomethyl ether, respectively. Their homo‐ and copolyethers were synthesized with BF3· Et2O/1,4‐butanediol and trifluoromethane sulfonic acid as initiator through cationic ring‐opening polymerization. The structure of the polymers was characterized by FTIR and1H NMR. The ratio of two repeating units incorporated into the copolymers is well consistent with the feed ratio. Regarding glass transition temperature (Tg), the DSC data imply that the resulting copolymers have a lower Tg than pure poly(ethylene oxide). Moreover, the TGA measurements reveal that they possess in general a high heat decomposition temperature. The ion conductivity of a sample (P‐AN 20) is 1.07 × 10?5 S cm?1 at room temperature and 2.79 × 10?4 S cm?1 at 80 °C, thus presenting the potential to meet the practical requirement of lithium ion batteries for polymer electrolytes. Copyright © 2005 Society of Chemical Industry  相似文献   

19.
A poly(imide benzoxazole) was prepared directly from trimellitic anhydride chloride and 2,2‐bis(3‐amino‐4‐hydroxyphenyl)hexafluoropropane (BisAPAF) monomers in a two‐step method. In the first step, a poly(hydroxyamide amic acid) precursor was synthesized by the low‐temperature solution polymerization in an organic solvent. Subsequently, thermal cyclodehydration of the poly(hydroxyamide amic acid) precursor at 350°C produced the corresponding poly(imide benzoxazole). The inherent viscosity of the precursor polymer was 0.22 dL/g. The cyclized poly(imide benzoxazole) showed a glass transition temperature (Tg) at 329°C and a 5% weight loss temperature at 530°C in nitrogen and at 525°C in air. The poly(imide benzoxazole) is amorphous as evidenced by the wide‐angle X‐ray diffraction measurement. The structures of the precursor polymer and the fully cyclized polymer were characterized by Fourier transform infrared (FTIR) and proton nuclear magnetic resonance spectroscopy (1H NMR). © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 88: 2388–2391, 2003  相似文献   

20.
Aryloxycarbonylphenyl acrylates and methacrylates were prepared by reacting 4‐acryloyloxybenzoyl chloride and 4‐methacryloyloxybenzoyl chloride with different phenols. They were homopolymerized using benzoyl peroxide as the initiator at 65°C in dimethylformamide. The polymers were characterized by IR and 1H–NMR spectra and size exclusion chromatography. Differential scanning calorimetry and polarizing optical microscopy studies revealed that the phenyl esters of poly(4‐acryloyloxybenzoic acid) and poly(4‐methacryloyloxybenzoic acid) did not show any liquid crystalline properties, but, the para‐aryl–substituted phenyl esters did exhibit mesophase properties in the temperature range of 98–265°C depending on the nature of the aryl substituent. Polymethacrylates exhibit higher Tg, and lower Tm and Ti than the polyacrylates having the same pendant mesogen. Thermogravimetric analyses have shown that the initial decomposition temperatures of the polymers are above 230°C. © 2000 John Wiley & Sons, Inc. J Appl Polym Sci 75: 465–474, 2000  相似文献   