Sugarcane pulp residue (SPR), a waste from sugar-refinery, which possesses a large surface area, can be used for removing
chromium (Cr(III) and Cr(VI)) from wastewater. In this work, the kinetics, isotherms of Cr(III) and Cr(VI) adsorption and
their removal by SPR were investigated. The results show that the removal percentages of Cr(VI) and Cr(III) increase with
increasing SPR dosage and temperature and decrease with increasing SPR particle size and the initial concentration of chromium
ions. However, the influence of pH value on the Cr(VI) removal differs from that of the Cr(III) removal. The Cr(VI) removal
percentage decreases with increasing pH values, while the Cr(III) removal percentage increases with increasing pH value. The
adsorption kinetics of Cr(VI) and Cr(III) well fits with pseudo-second-order model. Langmuir adsorption isotherm can well
describe the adsorption phenomena of chromium ions with the maximum adsorption capacity of 0.567 mg/g for Cr(VI) and 3.446
mg/g for Cr(III). Moreover, SPR reveals higher adsorption capacity for Cr(III) than that for Cr(VI), which implies that SPR
has more potential application for Cr(III)-containing wastewater treatment than that for Cr(VI)-containing wastewater treatment.
Foundation item: Projects(2006AA06Z374, 2007AA021304) supported by the National High-Tech Research and Development Program of China; Project(2008SK2007)
supported by the Key Program of Science and Technology of Hunan Province, China 相似文献
2.
3.
The adsorption of Ca(Ⅱ) ions from aqueous solution by chitosan α-ketoglutaric acid(KCTS) and hydroxamated chitosan α-ketoglutaric acid(HKCTS) was studied in a batch adsorption system.The Langmuir and Freundlich adsorption models were applied to describing the equilibrium isotherms,and isotherm constants were determined.The kinetics of the adsorption with respect to the initial Ca(Ⅱ) ions concentration,temperature and pH was investigated.The pseudo-first-order and second-order kinetic models were used to des... 相似文献
4.
The La-Mg-Ni-based A2B7-type La0.5Mg0.2Ni3.3Co0.2Six (x=0-0.2) electrode alloys were prepared by casting and annealing. The influences of the additional silicon and the annealing treatment on the structure and electrochemical performances of the alloys were investigated systemically. Both of the analyses of XRD and SEM reveal that the as-cast and annealed alloys are of a multiphase structure, involving two main phases (La, Mg)2Ni7 and LaNi5 as well as one minor phase LaNi3. The addition of Si and annealing treatment bring on an evident change in the phase abundances and cell parameters of (La, Mg)2Ni7 and LaNi5 phase for the alloy without altering its phase structure. The phase abundances decrease from 74.3% (x=0) to 57.8% (x=0.2) for the (La, Mg)2Ni7 phase, and those of LaNi5 phase increase from 20.2% (x~0) to 37.3% (x=0.2). As for the electrochemical measurements, adding Si and performing annealing treatment have engendered obvious impacts. The cycle stability of the alloys is improved dramatically, being enhanced from 80.3% to 93.7% for the as-annealed (950 ℃) alloys with Si content increasing from 0 to 0.2. However, the discharge capacity is reduced by adding Si, from 399.4 to 345.3 mA.h/g as the Si content increases from 0 to 0.2. Furthermore, such addition makes the electrochemical kinetic properties of the alloy electrodes first increase and then decrease. Also, it is found that the overall electrochemical properties of the alloys first augment and then fall with the annealing temperature rising. 相似文献