基金项目:国家自然科学基金项目,国家杰出青年基金资助,第四期江苏省省“333工程”培养资金资助项目“混凝土断裂有限元线法理论及其应用研究”
摘    要:为探讨不同尺寸混凝土三点弯曲梁试件断裂过程的差异性及其尺寸效应,设计了高度为0.25 m、0.30 m、0.40 m、0.50 m的4组16根不同尺寸混凝土三点弯曲梁试件,对其进行全过程断裂试验,并分析了荷载~张口位移曲线、起裂和失稳荷载、起裂和失稳韧度等断裂参数的变化。结合双K断裂韧度计算方法,得到不同尺寸混凝土三点弯曲梁试件的起裂韧度和失稳韧度。结果表明:不同尺寸混凝土试件断裂过程具有差异性;起裂韧度不随试件高度的增加而变化,失稳断裂韧度随试件高度的增加而增大。试件高度从0.25 m增加到0.50 m时,失稳韧度增加了0.40 MPa·m1/2。

关 键 词:混凝土弯曲梁  断裂试验  起裂韧度  失稳韧度  
收稿时间:2015-01-21

Experimental study on fracture process of various size specimens of three-point bending concrete beam
HU Shaowei,AN Kang.Experimental study on fracture process of various size specimens of three-point bending concrete beam[J].Water Resources and Hydropower Engineering,2015,46(6):120-125.
Authors:HU Shaowei  AN Kang
Affiliation:(Nanjing Hydraulic Research Institute,Nanjing210024,Jiangsu, China)
Abstract:Abstract:In order to study the discrepancies and their size effects of the fracture processes of various three-point bending concrete beams,4 group and 16 pieces of various three-point bending concrete beams with the heights of 0.25 m,0.30 m, 0.40 m and 0.50 m respectively are designed,and then the whole process fracture experiments are made for them,while the changes of the fracture parameters,such as load-opening displacement curve,cracking and destabilizing loads,cracking and destabilizing toughnesses,etc. are analyzed as well. In accordance with the calculation method for the double-K fracture toughness,both the cracking toughness and the destabilizing toughness of various three-point bending concrete beams are obtained. The result shows that discrepancies are there among the fracture processes of various three-point bending concrete beams; i.e. the cracking toughness is not changed along with the increase of the height of the specimen,while the destabilizing fracture toughness is increased along with the height of the specimen. When the height of the specimen is increased from 0.25 m to 0.50 m,the destabilizing toughness is increased by 0.40 MPa·m1/2.
Keywords:bending concrete beam  fracture experiment  cracking toughness  destabilizing toughness
本文献已被 CNKI 等数据库收录!
点击此处可从《水利水电技术》浏览原始摘要信息
点击此处可从《水利水电技术》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号