Process for improving the ladle free-opening rate for high aluminum steel in continuous casting
Authors:LIU Junzhan  ZHOU Tongjun  LUO Hui
Affiliation:Baosteel Special Steel Co.,Ltd,Shanghai 200940,China
Abstract:Steel 20Mn23AlV is a type of high aluminum steel with a very low ladle free-opening rate. The aluminum composition of 20Mn23AlV ranges from 1. 6% to 2. 45%,which is significantly higher than other types of steel.According to the real condition of 40 t ladle in steel-making plant of Baosteel Special Steel Company,previous works show that the key factors affecting the ladle free-opening rate of high aluminum steel in continuous casting are: sand material,accessories baking,ladle nozzle cleaning,the process and amount of adding sand,and the rate of argon stirring during refining. Therefore,improving the ladle filler sand quality,baking all of the raw materials,controlling the addition of ladle filler sand,cleaning the ladle nozzle,and optimizing argon stirring during the refining process can resolve the problem of a low ladle free-opening rate of high aluminum steel caused by the long ladle time of liquid steel.
Keywords:continuous casting  high aluminum steel  ladle  free-opening rate
本文献已被 CNKI 万方数据 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号