梅山选矿厂重选车间工艺流程分析及对策 |
| |
引用本文: | 杜建发.梅山选矿厂重选车间工艺流程分析及对策[J].工程设计与建设,2002(5). |
| |
作者姓名: | 杜建发 |
| |
作者单位: | 上海梅山矿业有限公司生产部 江苏南京210041 |
| |
摘 要: | 针对梅山选矿厂重选车间工艺流程使用 2 0多年来 ,尾矿平均品位高达 2 3 5 %~ 2 5 %的情况 ,通过技术改造 ,降低了尾矿品位与选矿比 ,提高了综合铁精矿的金属回收率 ,获得了较好的经济效益
|
关 键 词: | 铁矿 选矿 重选 技术改造 |
Analysis of process flow of gravity separation workshop and its countermeasures for Meishan concentrator |
| |
Authors: | DU Jian fa |
| |
Affiliation: | DU Jian fa |
| |
Abstract: | In view of the high average grade of tailing (23 5%~25%) during over 20 years of application of gravity separation process flow in Meishan concentrator in the past, the tailing grade and ore concentration ratio were reduced, the metal recovery of complex iron concentrate was improved and good economic benefits were obtained by technical modification |
| |
Keywords: | iron ore mineral processing gravity separation technical modification |
本文献已被 CNKI 等数据库收录! |
|