首页 | 官方网站   微博 | 高级检索  
     

聚乙烯及其复合管道安全检测与评价方法
引用本文:施建峰,郭伟灿,师俊,钟思嘉,郑津洋.聚乙烯及其复合管道安全检测与评价方法[J].化工学报,2013,64(2):756-764.
作者姓名:施建峰  郭伟灿  师俊  钟思嘉  郑津洋
作者单位:浙江大学化工机械研究所,浙江 杭州 310027
摘    要:聚乙烯及其复合管道广泛应用于油气输送、城市燃气等能源领域,其安全性至关重要。焊接接头的安全检测及评价是聚乙烯及其复合管道系统安全的关键技术。介绍了聚乙烯管道焊接接头的无损检测原理及方法、冷焊检测技术以及缺陷分类与失效模式三方面内容。对电熔和热熔焊接接头分别采用超声相控阵和耦合聚焦技术进行超声检测,并给出了缺陷剖切与检测结果的对比图。提出了物理概念清晰、工程应用方便的冷焊超声检测方法。将电熔接头中的缺陷分为熔合面缺陷、孔洞、结构畸变和过焊。分别对含不同类型和大小缺陷的电熔接头进行力学性能测试,发现电熔接头存在三种典型的失效模式,即沿电熔套筒壁贯穿裂纹失效、熔合面失效以及沿电阻丝所在平面贯穿裂纹失效。根据试验测试与理论分析结果,提出了相应的安全评定方法。所提出的方法,填补了国内外在聚乙烯管道安全检测与评价方法方面的技术空白,提高了燃气管道的本质安全性。

关 键 词:聚乙烯管  复合管  焊接接头  无损检测  安全评定  
收稿时间:2012-08-02
修稿时间:2012-09-05

Development of non-destructive testing and safety assessment of polyethylene and composite pipes
SHI Jianfeng , GUO Weican , SHI Jun , ZHONG Sijia , ZHENG Jinyang.Development of non-destructive testing and safety assessment of polyethylene and composite pipes[J].Journal of Chemical Industry and Engineering(China),2013,64(2):756-764.
Authors:SHI Jianfeng  GUO Weican  SHI Jun  ZHONG Sijia  ZHENG Jinyang
Affiliation:Institute of Process Equipment, Zhejiang University, Hangzhou 310027, Zhejiang, China
Abstract:Polyethylene (PE) and its composite pipes have been widely used in the transportation of energy, such as natural gas and petroleum.Pipe welding joints have been proven to be a weak link of the whole pipeline.This means that non-destructive testing (NDT) and safety assessment of these joints are key technologies to guarantee safety of pipeline.In this paper, the theory and method of NDT technology on welding joint of PE pipes, inspection technique of cold welding and safety assessment of welding joints containing defects are introduced.Ultrasonic phased array and coupling focusing technology are applied in the inspection of electrofusion and butt-fusion joints of PE pipes respectively.Figures with inspecting image and cross section of practical joint are given.A cold welding inspection method based on ultrasonic phased array technology was invented, which has clear physics concept and is convenient in application.The defects in the electrofusion joints of PE pipe are classified into four categories:poor fusion interface, over welding, voids and structural deformity.Mechanical tests of joints with different kind of defects show that there are three main failure modes of EF joint under inner pressure, that is, cracking through the fusion interface, cracking through the fitting, and cracking through copper wire interface.A safety assessment method was proposed based on the experimental and analytical results.The proposed method can greatly improve intrinsical safety of such pipeline.
Keywords:polyethylene pipe  composite pipe  welding joint  non-destructive testing  safety assessment
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《化工学报》浏览原始摘要信息
点击此处可从《化工学报》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23