Low-temperature synthetic route for boron carbide
Affiliation:1. CEA Saclay, DEN, DANS, DMN, SRMA, LA2M, Université Paris-Saclay, 91191, Gif/Yvette, France;2. CEA Saclay, DEN, DANS, DMN, SRMP, Laboratoire JANNUS, Université Paris-Saclay, 91191, Gif/Yvette, France;3. CNRS/IN2P3/IPNL, 69622, Villeurbanne, France;1. School of Metallurgy and Materials Science, Iran University of Science and Technology, P.O. Box 16845-161, Tehran, Iran;2. Department of Materials Science and Engineering, Shahreza Branch, Islamic Azad University, Isfahan, Iran;1. School of Materials Science and Engineering, Key Laboratory of Nonferrous Materials and New Processing Technology of Ministry of Education, Guilin University of Technology, Guilin 541004, China;2. Guangxi Key Laboratory in Universities of Clean Metallurgy and Comprehensive Utilization for Non-ferrous Metals Resources, Guilin University of Technology, Guilin 541004, China;3. The State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan 430070, China;1. Advanced Materials Research Center, Materials Engineering Department, Najafabad Branch, Islamic Azad University, Najafabad, Iran;2. Department of Materials Science and Engineering, Shahreza Branch, Islamic Azad University, Isfahan, Iran;3. MacDiarmid Institute for Advanced Materials and Nanotechnology, Victoria University of Wellington, New Zealand
Abstract:Boron carbide is one of the hardest materials with diamond-like mechanical properties, and is already used for a variety of applications including armor plating, blasting nozzles, and mechanical seal faces, as well as for grinding and cutting tools. It is produced on an industrial scale by classical carbothermal reduction of boric oxides at high temperatures, but the formation of pure boron carbide in processed forms, such as films and fibers, is difficult. As an alternative to high-temperature powder techniques, there is recently great interest in the development of polymer precursors to produce ceramic materials. The aim of the present work is to develop a cost effective and low-temperature manufacturing process to synthesize boron carbide from cheap and easily available raw materials. The initial objective of our research is the design and synthesis of a new type of boron–carbon polymer, which would serve as precursor for boron carbide. The polymeric precursor is synthesized by the reaction of boric acid and polyvinyl alcohol that after pyrolysis at 400 °C and 800 °C gives boron carbide. The polymeric precursor and its pyrolyzed products are characterized by Fourier transform infrared spectroscopy (FTIR) and X-ray diffraction (XRD). X-ray diffraction shows that boron carbide (B4C) obtained from this method has an orthorhombic crystal structure. It is a unique low-temperature (~400 °C) synthetic route for boron carbide.
Keywords:
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号