SPHD薄板坯连铸漏钢原因分析及控制措施
引用本文:杜洪波,杨杰.SPHD薄板坯连铸漏钢原因分析及控制措施[J].中国冶金,2007,17(6):59-59.
作者姓名:杜洪波  杨杰
作者单位:唐山钢铁股份有限公司第一钢轧厂,河北 唐山 063016
摘    要:分析了唐钢FTSC薄板坯连铸机生产低碳冷轧用钢过程中漏钢的成因;提出了优化锥度控制、改进结晶器窄面铜板形状和优化水口形状等技术措施。这些措施实施后,低碳钢生产过程中的漏钢得到有效控制。

关 键 词:FTSC薄板坯连铸机    低碳冷轧用钢    锥度控制    铜板形状    水口形状  
文章编号:1006-9356(2007)06-0059-04
修稿时间:2007-04-04

Causes and Countermeasures of Breakout During Production of SPHD by Thin Slab Casting in Tanggang
DU Hong-bo,YANG Jie.Causes and Countermeasures of Breakout During Production of SPHD by Thin Slab Casting in Tanggang[J].China Metallurgy,2007,17(6):59-59.
Authors:DU Hong-bo  YANG Jie
Affiliation:No.1 Steel Making and Rolling Plant, Tangshan Iron and Steel Group Co Ltd,Tangshan 063016,Heibei,China
Abstract:The causes of breakout during the production of low carbon steel for cold rolling by Tanggang FTSC thin slab caster were analysed and the optimization countermeasures such as the control of mould taper, the copper plate shape of mould narrow side and SEN shape were put forward. With the respective measures, the breakout has been avoided.
Keywords:FTSC thin slab caster  low carbon steel for cold rolling  mould taper control  copper plate shape  SEN shape