摘 要: | 探讨了花园岭四号铅锌矿矿石的可选性,确定浮选工艺条件,采用优先浮选流程,最终闭路试验获得,铅精矿品位56.63%、铅回收率70.70%,锌精矿品位55.76%、锌回收率90.92%,硫精矿品位49.50%、硫回收率81.68%的试验指标,其中锌精矿、硫精矿均为一级品。
|
关 键 词: | 优先浮选 铅锌分离 组合抑制剂 |
文章编号: | 1671-9492(2005)02-0013-04 |
修稿时间: | 2004年11月18 |
THE MINERAL SEPARATION TEST RESEARCH FOR HUAYUANLING NO.4 LEAD AND ZINC MINE IN SUICHANG |
| |
Authors: | WANG Yun-feng HE Bing-lin NI Yan-qun |
| |
Abstract: | The selective possiblity of Huayuanling No.4 lead and zinc mine is discussed. The flotation industrial condition is fixed. The selective-flotation flowsheet is adopted,and from the final closed circuit test index of the following products is obtained:lead-concentrate βPb56.63%?εPb70.70%;zinc-concentrate βZn55.76%?εZn90.92%;sulfur-concentrate βs49.50%?εs81.68%,of which zinc-concentrate and sulfur-concentrate are both top products. |
| |
Keywords: | selective-flotation lead and zinc disintegration combined depresent |
本文献已被 CNKI 维普 万方数据 等数据库收录! |
| 点击此处可从《有色金属(选矿部分)》浏览原始摘要信息 |
|
点击此处可从《有色金属(选矿部分)》下载全文 |
|