Influence of NaCl-CaCl2 on Decomposing REPO4 with CaO
Authors:Sun  Wu Zhiying  Bian Xue  Gao Bo  Wu Wenyuan  Tu Ganfeng
Affiliation:

aSchool of Materials & Metallurgy, Northeastern University, Shenyang 110004, China

Abstract:The influence of NaCl-CaCl2 on thermal decomposition of REPO4(RE: Ce, La, Nd, Th) with CaO was studied. The heat decomposing process of REPO4 was tested with TG-DTA experiments. The results showed that the decomposition temperature of REPO4 with CaO was reduced because of adding NaCl-CaCl2 mixture (NaCl:CaCl2 = 1:1). The influence of the addition of NaCl-CaCl2, roasting temperature and roasting time on decomposition ratio of REPO4 with CaO was studied. The results showed that the decomposition ratio of REPO4 with CaO was 79% when the addition percentage of NaCl-CaCl2, was 10%, the roasting temperature was 150°C, and the roasting time was 1 h.
Keywords:NaCl-CaCl2  CaO  REPO4  decomposition ratio  rare earths
本文献已被 维普 万方数据 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号