提高160t钢包自开率的工艺实践 |
| |
引用本文: | 陈永金,陆志坚,杨剑洪.提高160t钢包自开率的工艺实践[J].柳钢科技,2011(2). |
| |
作者姓名: | 陈永金 陆志坚 杨剑洪 |
| |
作者单位: | 转炉炼钢厂; |
| |
摘 要: | 系统分析造成160t钢包不能自动开浇的主要原因:引流砂烧结过度和水口底部结冷钢。总结了提高引流砂质量的措施,实施后月平均自开率达到98.81%。
|
关 键 词: | 炼钢 连铸 钢包 自开率 引流砂 |
Process Practice on Improving Auto-casting Ratio of 160 t Ladle |
| |
Authors: | CHEN Yong-jin LU Zhi-jian YANG Jian-hong |
| |
Affiliation: | CHEN Yong-jin LU Zhi-jian YANG Jian-hong (Converter Steel-making) |
| |
Abstract: | The main causes of drainage sand over-sintering and steel solidified in the nozzle bottom resulting in 160 t ladle cannot cast automatically were analyzed systematically. The measures of improving drainage sand quality were summarized and the average auto-casting ratio can reach 98.81 % after implement of measures. |
| |
Keywords: | Steelmaking Continuous Casting Ladle Auto-casting Ratio Drainage Sand |