加工高酸原油常减压装置高温腐蚀分析及对策
引用本文:闻明科.加工高酸原油常减压装置高温腐蚀分析及对策[J].广东化工,2009,36(9):191-193.
作者姓名:闻明科
作者单位:中海石油炼化有限责任公司,惠州炼油分公司,广东,惠州,516086
摘    要:惠州炼油项目拟加工蓬莱19-3原油,该原油属于高酸低硫中间环烷基原油,文章根据环烷酸腐蚀的特点及其影响因素,提出了环烷酸腐蚀环境的选材建议,并依据惠州炼油项目常减压工艺流程图分析了惠州炼油项目常减压装置环烷酸腐蚀的重点部位。

关 键 词:高酸原油  腐蚀  环烷酸  常减压装置

The Analysis and Countermeasure for the Crude Oil with High TAN in CDU
Wen Mingke.The Analysis and Countermeasure for the Crude Oil with High TAN in CDU[J].Guangdong Chemical Industry,2009,36(9):191-193.
Authors:Wen Mingke
Affiliation:Wen Mingke (Huizhou Refinery of the CNOOC Petrochemical and Oil Co., Ltd., Huizhou 516086, China)
Abstract:The Penglai19-3 crude oil(PL19-3 in brief), the feed stock of Huizhou Refinery CDU, is characteristic of the naphthene middle crude oil with low content sulfur and high TAN. For the corrosion of PL19-3, the material for the CDU must be chosen under the special condition of the PL19-3 corrosion, and the key part corroded by the napthenic acid will be analyzed with the art flow from the Huizhou Refinery.
Keywords:crude oil with high TAN  corrosion  naphthenic acid  CDU