摘    要:采用一段焙烧-酸浸-氰化工艺处理某复杂银精矿,结果表明:在焙烧温度923 K,焙烧时间2 h,酸浸反应液固比1.5∶1,反应pH 值为0.8~1.0,反应温度368 K,反应时间1.5 h,氰化反应液固比2∶1,反应pH 值为10~11,NaCN 浓度1.5 ‰,反应时间48 h 条件下,氰化浸出时Au、Ag 的浸出率分别为72.01 %、18.41 %,尾渣银含量355 g/t.在复杂银精矿与其它矿样按一定比例重新配矿后,采用相同试验条件,氰化时Au、Ag 的浸出率分别提高24.89 %、15.66 %,尾渣中银含量降低了223.35 g/t. 

关 键 词:焙烧   酸浸   氰化   复杂银精矿   配矿
收稿时间:2013-08-17

Extracting process of gold and silver from a complex silver concentrate
ZENG Bin,XIE Bo-yi,WANG Rui-xiang,yu Pan,MAO Ji-yong,WANG Zhi-gang,RUAN Jian-guo. Extracting process of gold and silver from a complex silver concentrate[J]. Nonferrous Metals Science and Engineering, 2013, 4(6): 28-32. DOI: 10.13264/j.cnki.ysjskx.2013.06.020
Authors:ZENG Bin  XIE Bo-yi  WANG Rui-xiang  yu Pan  MAO Ji-yong  WANG Zhi-gang  RUAN Jian-guo
Affiliation:1.School of Metallurgical and Chemical Engineering, Jiangxi University of Science and Technology, Ganzhou341000, China2.Nerin Engineering Company Limited, Nanchang 330031, China
Abstract:Roasting-acid leaching-cyanided process is adopted to treat the complex silver concentrate. The result shows that the cyanide leaching rate of gold and silver are 72.01% and 18.41% respectively, with the silver content of 355 g/t in residue, under the condition that roasting temperature is 923 K with roasting time of 2 h, sulfuric acid leaching liquid-solid ratio of 1.5:1, reaction pH value of 0.8 ~1.0, acid leaching temperature of 368 K with reaction time of 1.5 h, cyanided liquid-solid ratio of 2:lwith reaction pH value of 10~11, sodium cyanide concentration of 1.5 %0 with reaction time of 48 h. Under the same conditions, when complex silver concentrate blended with other mineral secondary ore according to certain proportion, the cyanide leaching rate of gold and silver raises by 24.89 % and 15.66 % respectively. The silver content reduces by 223.35 g/t in residue.
Keywords:roasting  acid leaching  cyanided  complex silver concentrate  ore blending
本文献已被 维普 等数据库收录!
点击此处可从《有色金属科学与工程》浏览原始摘要信息
点击此处可从《有色金属科学与工程》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号