Simultaneous formation of p- and n-type ohmic contacts to 4H-SiC using the ternary Ni/Ti/Al system
Authors:S Tsukimoto  T Sakai  T Onishi  Kazuhiro Ito  Masanori Murakami
Affiliation:(1) Department of Materials Science and Engineering, Kyoto University, 606-8501 Kyoto, Japan
Abstract:Fabrication procedures for silicon carbide power metal oxide semiconductor field effect transistors (MOSFETs) can be improved through simultaneous formation (i.e., same contact materials and one step annealing) of ohmic contacts on both the p-well and n-source regions. We have succeeded with the simultaneous formation of the ohmic contacts for p- and n-type SiC semiconductors by examining ternary Ni/Ti/Al materials with various compositions, where a slash symbol “/” indicates the deposition sequence starting with Ni. The Ni(20 nm)/Ti(50 nm)/Al(50 nm) combination provided specific contact resistances of 2 × 10−3 Ω-cm2 and 2 × 10−4 Ω-cm2 for p- and n-type SiC, respectively, after annealing at 800°C for 30 min, where the doping level of Al in the SiC substrate was 4.5 × 1018 cm−3 and the level of N was 1.0 × 1019 cm−3.
Keywords:4H-SiC  Ni/Ti/Al  ohmic contact  simultaneous formation
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号