摘    要:当超临界直流锅炉燃用煤的硫含量St.ar平均值在1.5%以上时,一般会出现高温腐蚀。通过对某超临界前、后墙对冲燃烧直流锅炉所送检的水冷壁管烟气侧腐蚀状况,采用目视、体视镜、电镜、能谱以及X射线衍射分析等方法进行检查分析,确定了高温硫腐蚀的产物,并对成因进行分析,然后提出防治的措施和建议,为预防高温硫腐蚀提供参考。

关 键 词:超临界  直流锅炉  水冷壁管  高温硫腐蚀  能谱分析  X射线衍射分析
收稿时间:2010-03-22
修稿时间:2010-03-25

Causes and Prevention of High Temperatures Sulfur Corrosion of Water Wall Tubes of Supercritical Concurrent Boiler
HE Yong-bing,WANG Wei-jun,LI Chang-ming,HE Jun-feng,SUN Hou-li.Causes and Prevention of High Temperatures Sulfur Corrosion of Water Wall Tubes of Supercritical Concurrent Boiler[J].Electric Power Construction,2010,31(10):61-66.
Authors:HE Yong-bing  WANG Wei-jun  LI Chang-ming  HE Jun-feng  SUN Hou-li
Affiliation:1.Hebi Fenghe Power Generation Co.Ltd.,Hebi 458008,Henan Province,China;2.Wuhan University,Wuhan 430072,China;3.Henan Electric Power Test Research Institute,Zhengzhou 450007,China)
Abstract:When the content of sulfur St.ar is more than 1.5% in the coal,high temperature sulfur corrosion will generally occur in supercritical concurrent boilers.An analysis is made of the corroded water wall samples of a supercritical concurrent boiler by such means as visual inspection,stereoscope,electron microscope,energy spectrum and X ray diffraction,and the production of high temperature sulfur corrosion is determined.Based on the analysis of the causes for the corrosion,some prevention measures are proposed,which can be used as a reference for prevention of high temperature sulfur corrosion.
Keywords:supercritical  concurrent boiler  water wall tube  high temperature sulfur corrosion  energy spectrum analysis  X ray diffraction analysis