研究了以管沟污泥等量替代天然细集料制备水泥混凝土的技术。结果表明,在混凝土中掺加一定量的管沟污泥可以配制出强度为40MPa以上的混凝土,同时其28d强度可高于同配合比的基准混凝土。此外,随污泥掺量的增加,混凝土坍落度会降低,凝结时间会延长。测试掺污泥的水泥混凝土固结体中重金属溶出量表明其可满足国家标准的要求,无二次污染。 相似文献
52.
53.
基于静载试验的RC桥梁承载力评估 总被引:1,自引:0,他引:1
即有桥梁承载力的评估方法众多,而静载试验法可以对即有混凝土桥梁承载力做到准确、高效地评估.确定了某桥的静载试验方案,并将试验数据和有限元模拟数据相比较,对其承载力进行评估. 相似文献
54.
从国产耐候钢S355J2W着手,选用同类别的进口耐候钢SMA490BW作为对比,匹配2种焊丝ISO 14341-AG424M21Z和CHW-55CNH,形成3种接头,对这3种接头分别进行疲劳试验,并从试验数据、宏观形貌及断口显微形貌进行分析,对比3种接头的疲劳性能。 相似文献
55.
56.
A gas-dissolving device was designed and connected to the falling-body viscometer, which was used to determine the viscosities of liquids in our lab before. The equipment can be used to determine the gas composition, the densities and viscosities of the solution at the same time. The densities and viscosities of [bmim][PF6] + CO2 binary system were determined in the temperature range of 313.2 to 413.2 K and pressure range of 5.0 to 25.0 MPa by the equipment. Then the viscosities of [bmim][PF6] + CO2 binary system at constant temperature, constant pressure, and different temperature and pressure were correlated, respectively. For the correlation at different tempera- ture and different t3ressure for different concentration mixtures the average relative deviation ARD is 0.037. 相似文献
57.
GIS电流互感器超差原因分析 总被引:1,自引:0,他引:1
以试验数据证实了500 kV GIS电流互感器在安装后出现的超差问题,并从理论上阐述了造成互感器超差的原因,且给出了解决方案。 相似文献
58.
腐蚀蚀坑是索承式桥梁吊索力学性能退化的主要原因。基于断裂力学和蚀坑等效,考虑腐蚀蚀坑影响,以吊索在荷载作用下的安全系数小于2.5作为吊索失效判据,建立腐蚀吊索承载力安全性能评估方法,并以袁州大桥钢丝腐蚀速率数据为基础,进行参数敏感性分析和算例计算,研究了各工况下吊索失效时的断丝数量和安全系数小于2.5的时间。结果表明,该方法相比较均匀腐蚀理论模型,考虑了钢丝腐蚀蚀坑对吊索承载力的影响,能够预测钢丝断裂数量和安全系数小于2.5的时间。 相似文献
59.