首页 | 官方网站   微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 578 毫秒
1.
Poly(N‐vinyl pyrrolidone) (PVP) and poly (vinyl alcohol) (PVA) homopolymers and their blended samples with different compositions were prepared using cast technique and subjected to X‐ray diffraction (XRD) measurements, infrared (IR) spectroscopy, ultraviolet/visible spectroscopy, and thermogravimetric analysis (TGA). XRD patterns of homopolymers and their blended samples indicated that blending amorphous materials, such as PVP, with semicrystalline polymer, such as PVA, gives rise to an amorphous structure with two halo peaks at positions identical to those found in pure PVP. Identification of structure and assignments of the most evident IR ‐ absorption bands of PVP and PVA as well as their blends in the range 400–2000 cm?1 were studied. UV–vis spectra were used to study absorption spectra and estimate the values of absorption edge, Eg, and band tail, Ee, for all samples. Making use of Coats‐Redfern relation, thermogravimetric (TG) data allowed the calculation of the values of some thermodynamic parameters, such as activation energy E, entropy ΔS#, enthalpy ΔH, and free energy of activation ΔG# for different decomposition steps in the samples under investigation. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009  相似文献   

2.
In this work we studied the electrical behavior of Linde type A zeolite (K+) in the presence of two polymers, poly(vinyl alcohol) (PVA) and poly(vinyl pyrrolidone) (PVP), with excellent film forming properties. Homogeneous composite thin films of PVA/LTA‐zeolite and PVP/LTA‐zeolite were prepared with different zeolite concentrations. The current?voltage (I?V) characteristics of the composites were measured at different applied voltages. The results show that the conductivity properties are composition‐ratio‐dependent and are also related to the type of polymers. Moreover, a well‐defined step‐like change was detected in the I?V curve of PVP/LTA‐zeolite at very high applied voltage. © 2013 Society of Chemical Industry  相似文献   

3.
Poly(vinyl alcohol)/poly(N‐vinyl pyrrolidone) (PVP)/chitosan hydrogels were prepared by a low‐temperature treatment and subsequent 60Co γ‐ray irradiation and then were medicated with ciprofloxacin lactate (an antibiotic) and chitosan oligomer (molecular weight = 3000 g/mol). The gel content, swelling ratio, tensile strength, and crystallinity of the hydrogels were determined. The effects of the chitosan molecular weight, the low‐temperature treatment procedure, and the radiation dosage on the hydrogel properties were examined. The molecular weight of chitosan was lowered by the irradiation, but its basic polysaccharide structure was not destroyed. Repeating the low‐temperature treatment and γ‐ray irradiation caused effective physical crosslinking and chemical crosslinking, respectively, and contributed to the mechanical strength of the final hydrogels. The incorporation of PVP and chitosan resulted in a significant improvement in the equilibrium swelling ratio and elongation ratio of the prepared hydrogels. The ciprofloxacin lactate and chitosan oligomer were soaked into the hydrogels. Their in vitro release behaviors were examined, and they were found to follow diffusion‐controlled kinetics. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 2453–2463, 2006  相似文献   

4.
Poly(ethylene‐co‐vinyl alcohol)/poly(vinyl pyrrolidone) (EVAL/PVP) blend membranes with antifouling properties were prepared by nonsolvent induced phase separation. Residual PVP in the sample was calculated by infrared spectroscopic data and confirmed by thermogravimetric analysis. The effect of residual PVP on hydrophilicity and permeation characteristics of the membranes was evaluated. Porosity and equilibrium water content of the membranes were influenced by the addition of PVP. The effect of protein fouling on flux using bovine serum albumin as a model system was studied in detail. The residual PVP content could enhance the antifouling property of the membrane. All membranes proved to have sufficient mechanical strength to withstand pressure‐driven filtrations.  相似文献   

5.
Biocompatible and easily available materials from dairy production waste were used for modification of water‐soluble polymeric blends of Poly(vinyl alcohol) (PVA) and Poly(vinyl pyrrolidone) (PVP). The resulting biocomposites of PVA/PVP with various concentrations of lactose (L) or calcium lactate (CL) (0, 5, 15, 25, 35 wt%) were prepared by using a solvent cast technique and then characterized by optical microscopy, tensile test, water content determination, differential scanning calorimetry (DSC), Fourier transform infrared spectroscopy equipped by attenuated total reflectance device, and also tested for biodegradability. The films were transparent with a smooth surface. The results confirm that L and CL work as fillers in polymeric matrix. The tensile investigations showed enhanced Young's modulus (E) and tensile strength for low‐filled of composite materials (up to 5 wt% L and 15 wt% CL). The biodegradation test in aquatic conditions revealed improved biodegradability of modified blends. Both L and CL seem to be suitable for the modification of polymers, which can be convenient from economical and environmental point of view. POLYM. COMPOS., 27:147–152, 2006. © 2006 Society of Plastics Engineers.  相似文献   

6.
A controlled‐release preparation of diclofenac sodium for transdermal administration has been developed. Poly(vinyl alcohol) (PVA) and PVA/poly(acrylic acid) (PAA) alloy membranes were prepared from a solvent‐casting technique using different PVA/PAA (v/v) ratios. The release of the drug from the membrane was evaluated under in vitro conditions at pH 7.4. The delivery system provided linear release without time lag, burst effect, and boundary layer resistance. Effects of variables such as film thickness and PVA/PAA ratio on the permeation behavior of the polymeric membranes were discussed. The optimal PVA/PAA was determined as 50/50. © 2003 Wiley Periodicals, Inc. J Appl Polym Sci 91: 72–77, 2004  相似文献   

7.
In this study, itaconic acid (IA) was grafted on poly(vinyl alcohol) (PVA) at two different grafting percentages, 7.0% (w/w) and 14.0% (w/w), and membranes were prepared from the grafted copolymer (PVA‐g‐IA). Performances of PVA and PVA‐g‐IA membranes for the transdermal release of salicylic acid (SA) at in vitro conditions were investigated by using 2.0 mg/mL SA solutions. Effect of the pH on the release of SA was studied by keeping pH of donor and acceptor solutions in a range of (2.1–7.4). Permeation studies were also carried on at different SA concentrations. Effect of temperature on the release of SA was investigated in the temperature range of (32–39) (±1)°C. Results showed that presence of IA decreased the release of SA from the PVA membranes and 73% SA was released at the end of 48 h at (32 ± 1)°C from the IA‐1 membranes. pH affected the release of SA through the grafted membranes and studies showed that release of SA was high with donor solution pH of 2.1. When the pH of donor and receiver solutions were kept at the same pH value, the overall SA% in permeate increased. Increase in concentration of SA decreased the release of SA for the studied membranes. Release of SA from PVA‐g‐IA membranes was temperature sensitive and increase in temperature from (32 ± 1)°C to (39 ± 1)°C increased the release percentage of SA by 24% (w/w). The overall activation energy for the permeation of SA through IA‐1 membrane was found to be 22.97 kJ/mol. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2008  相似文献   

8.
In this study, acrylamide (AAm) was grafted onto poly(vinyl alcohol) (PVA) in solution with UV radiation, and membranes were prepared from the graft copolymer (PVA‐g‐AAm) for transdermal release of salicylic acid (SA) at in vitro conditions. Permeation studies were carried out using a Franz‐type diffusion cell. Release characteristics of SA through PVA and PVA‐g‐AAm membranes were studied using 2.0 mg/mL SA solutions. Effects of the presence of AAm in the copolymer, pH of donor and acceptor solution, and concentration of SA and temperature on the release of SA were investigated. Permeation of SA through the membranes was found to be pH‐dependent, and increase in pH generally increased the release percentage of SA, and the presence of AAm in the membrane positively affected the permeation. The effect of concentrations of SA on the permeation was also searched using saturated solution of SA, and permeated amount of SA was found to be less than in the case of unsaturated SA solution. Studies showed that the release of SA from PVA‐g‐AAm membranes was temperature‐sensitive and increase in temperature increased the permeation rate. 82.76% (w/w) SA was released at the end of 24 h at (39 ± 1)°C, and the overall activation energy for the permeation of SA through PVA‐g‐AAm membranes was found to be 19.65 kJ/mol. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2008  相似文献   

9.
The structure and performance of modified poly(vinylidene fluoride‐co‐hexafluoropropylene) (PVdF‐co‐HFP) ultra‐filtration membranes prepared from casting solutions with different concentrations of poly(vinyl pyrrolidone) (PVP) were investigated in this study. Membrane properties were studied in terms of membrane compaction, pure water flux (PWF), water content (WC), membrane hydraulic resistance ( R m), protein rejection, molecular weight cut‐off (MWCO), average pore size, and porosity. PWF, WC, and thermal stability of the blend membranes increased whereas the crystalline nature and mechanical strength of the blend membranes decreased when PVP additive concentration was increased. The contact angle (CA) decreased as the PVP concentration increased in the casting solution, which indicates that the hydro‐philicity of the surface increased upon addition of PVP. The average pore size and porosity of the PVdF‐co‐HFP membrane increased to 42.82 Å and 25.12%, respectively, when 7.5 wt% PVP was blended in the casting solution. The MWCO increased from 20 to 45 kDa with an increase in PVP concentration from 0 to 7.5 wt%. The protein separation study revealed that the rejection increased as the protein molecular weight increased. The PVdF‐co‐HFP/PVP blended membrane prepared from a 7.5 wt% PVP solution had a maximum flux recovery ratio of 74.3%, which explains its better antifouling properties as compared to the neat PVdF‐co‐HFP membrane. POLYM. ENG. SCI., 55:2482–2492, 2015. © 2015 Society of Plastics Engineers  相似文献   

10.
Poly(acrylonitrile‐coN ‐vinyl‐2‐pyrrolidone)s (PANCNVPs) show excellent biocompatibility. In this work, PANCNVPs with different contents of N‐vinyl‐2‐pyrrolidone (NVP) were fabricated into asymmetric membranes by the phase inversion method. The surface chemical composition of the resultant membranes was determined by Fourier transform infrared spectroscopy–attenuated total reflection. Field emission scanning electron microscopy was used to examine the surface and cross section morphologies of the membranes. It was found that the morphologies hardly change with the increase of NVP content in PANCNVP, while the deionized water flux increases remarkably and the bovine serum albumin (BSA) retention decreases slightly. Experiment of dynamic BSA solution filtration was carried out to evaluate the antifouling properties of the studied membranes. The relative flux reduction of PANCNVP membrane containing 30.9 wt % of NVP is 25.9%, which is far smaller than that of the polyacrylonitrile membrane (68.8%). Results deduce that this improvement comes from the excellent biocompatibility of NVP moieties instead of the hydrophilicity change, because the water contact angles of these membranes fluctuate between 60 and 70°. Results from the membranes using poly(N‐vinyl‐2‐pyrrolidone) (PVP) as an additive confirm that, to a certain extent, the PANCNVP membranes show the advantages of antifouling compared with the polyacrylonitrile/PVP blending membrane. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 102: 4577–4583, 2006  相似文献   

11.
In this study, hydrogels were prepared from blends of poly(vinyl alcohol) (PVA) and poly(vinyl pyrrolidone) (PVP). The miscibility of the polymers was confirmed with differential scanning calorimetry with the appearance of a single glass‐transition temperature. Additionally, a negative Flory–Huggins interaction parameter further verified the interaction between PVA and PVP. We evaluated the stability of the hydrogels by swelling the gels in phosphate‐buffered saline solutions at pH 7.4. With attenuated total reflectance‐Fourier transform infrared spectroscopy, it was determined that, during swelling, PVP dissolved out of the gel over time and the equilibrium gel content of PVP was nearly identical in all of the samples investigated. After the dissolution of PVP, the equilibrium water content of the gels ranged from 64 to 76 wt %. Additionally, rubber elasticity studies were performed to elucidate information about the physically crosslinked network structure. As determined from rubber elasticity experiments, the mesh size of the physically crosslinked hydrogels ranged from 90 to 230 Å. © 2009 Wiley Periodicals, Inc. J Appl Polym Sci, 2009  相似文献   

12.
Tough biodegradable films were prepared using a poly(vinyl alcohol) (PVA)/poly(vinyl pyrrolidone) (PVP) (1:1) blend with plasticizers of glycerol (GLY), sorbitol (SOR), and their (one to one) mixture. We studied the effect of plasticization on the structural, thermal, and mechanical properties of the PVA/PVP blend films. Fourier transform infrared spectra indicated good miscibility of the two components due to the H‐bonding between the PVA and PVP molecules. The addition of plasticizers reduced the interaction between PVA and PVP, evidenced by an increase in the intensity of PVA diffraction peaks observed in the X‐ray diffraction (XRD) characterization. Thermal degradation of the blends increased as a function of the plasticizer used. GLY affected thermal degradation more than SOR and the mixtures. The incorporation of the plasticizers promoted the growth of PVA crystals as evidenced by XRD patterns and the enthalpy of fusion (ΔHf) obtained by differential scanning calorimetry measurements. The introduction of SOR to the binary blend increased toughness seven times and imparted simultaneous and pronounced improvements to maximum tensile stress and elongation at break. This behavior holds out great promise for the development of a new generation of mechanically robust, yet thoroughly biodegradable materials that could effectively supplant conventional polymers in demanding applications. © 2018 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2018 , 135, 46406.  相似文献   

13.
Transient currents (charging and discharging currents) in poly(vinyl alcohol) (PVA)–poly(vinyl pyrrolidone) (PVP) polymer blend films were measured over the temperature range 30–150°C at field strengths of 2.32–23.2 × 106 Vm?1. Polymer films were prepared by the isothermal immersion technique. Activation energies were evaluated from quasi-steady-state currents. A single relaxation peak was observed both from isochronal currents and low frequency dielectric relaxation. Activation energies evaluated from these two methods are found to be in fairly good agreement. The polarization is considered to be due to space charge origin along with some contribution from dipolar groups. The maximum loss was observed in Sample I (PVA: PVP = 25:75), suggesting maximum heterogeneity in this blend ratio.  相似文献   

14.
Poly(vinyl alcohol) (PVA) was chosen as a controllable gelator to prepare sodium alginate (SA)‐based physically cross‐linked dual‐responsive hydrogel by three steps. First, polyvinyl acetate (PVAc) was grafted onto SA via radical copolymerization. Then, the copolymer was subsequently converted into SA‐g‐poly(vinyl alcohol) (SAPVA) by alcoholysis reaction. PVA content of SAPVA was tailored by controlling the graft percentage of PVAc, i.e. through varying the amount of vinyl acetate during copolymerization. Finally, SAPVA hydrogels were formed by freezing‐thawing cycles. The structure of the graft copolymers was verified with FTIR spectroscopy. X‐ray diffraction analysis results revealed that the crystallinity of SAPVA hydrogels depended on the PVA content of SAPVA. The swelling test showed that SAPVA hydrogels were pH‐responsive, and the swelling was reversible. SAPVA hydrogels also behaved electric‐responsive. In addition, the pH‐sensitivity of SAPVA hydrogels was able to be controlled with the composition of the hydrogels. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2012  相似文献   

15.
Poly(vinylidene fluoride) (PVDF) powders were grafted with N‐vinyl pyrrolidone using the pre‐irradiation induced graft polymerization technique. The effects of reaction time, absorbed dose, and monomer concentration on the degree of grafting were investigated, and the grafted PVDF powders were characterized by Fourier transform infrared spectroscopy, thermogravimetric analysis, and differential scanning calorimetry. The grafted PVDF powders were also cast into microfiltration (MF) membranes via the phase‐inversion method. The contact angle and water uptake were measured. The membrane morphology was studied by scanning electron microscopy, and the water filtration properties of the membranes were tested. The antifouling properties were determined through measurements of the recovery percentage of pure water flux after the MF membranes were fouled with bovine serum albumin solution. The results confirmed that the existence of poly(N‐vinyl pyrrolidone) (PVP) graft chains improved the hydrophilicity and antifouling properties of the MF membranes cast from PVDF‐g‐PVP powders. © 2012 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2013  相似文献   

16.
Polymeric blend microspheres of poly(vinyl pyrrolidone) (PVP) with sodium alginate (NaAlg) were prepared by cross‐linking with calcium ions and used to deliver a calcium channel blocker drug, diltiazem hydrochloride (DT). The prepared microspheres were characterized by Fourier transform infrared spectroscopy and scanning electron microscopy. Scanning electron microscopy confirmed the spherical nature of the particles. Preparation conditions for the microspheres were optimized by considering the percentage entrapment efficiency, particle size, and swelling capacity. Effects of variables such as PVP/NaAlg ratio, molecular weight of PVP, cross‐linker concentration, and drug/polymer ratio on the release of DT were discussed at two different pH values (1.2, 6.8) at 37°C. It was observed that DT release from the microspheres decreased with increasing molecular weight of PVP and extent of cross‐linking. However, DT release increased with increasing PVP content and drug/polymer ratio (d/p) of the blend microspheres. The highest DT release percentage was obtained as 99% for PVP/NaAlg ratio of 1/2 with d/p ratio of 1/2 at the end of 4 h. It was also observed from release results that DT delivery from the microspheres through the external medium are much higher at low pH (1.2) value than that of high pH (6.8) value. The drug release from the microspheres mostly followed Fickian transport. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2008  相似文献   

17.
The miscibility behavior of ternary blends of poly (vinyl phenol) (PVPh)/poly (vinyl pyrrolidone) (PVP)/poly (ethyl methacrylate) (PEMA) was investigated mainly with calorimetry. PVPh is miscible with both PVP and PEMA on the basis of the single Tg observed over the entire composition range. FTIR was used to study the hydrogen bonding interaction between the hydroxyl group of PVPh and the carbonyl group of PVP and PEMA at various compositions. Furthermore, the addition of PVPh is able to enhance the miscibility of the immiscible PVP/PEMA and eventually transforms it into a miscible blend, especially when the ratio between PVP/PEMA is 3:1, probably because of favorable physical interaction. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 1205–1213, 2006  相似文献   

18.
Nanocomposites of aluminocilicate are of growing interest not only because they offer exceptional reinforcement at very low filler concentrations, but also because of their electromagnetic properties and natural origin. Aluminosilicate‐filled biodegradable composites of poly(vinyl alcohol) (PVA) and poly(vinyl pyrrolidone) (PVP) were prepared by a conventional solvent casting technique using glass plates as the casting surfaces. The aluminosilicate used in this study is a multicomponent natural clay material. Its average particle size is 23–24 nm. The dielectric and magnetic properties of composite materials of PVA‐PVP and aluminosilicate were investigated in wide frequency ranges from 1 MHz to 1 GHz. The complex permittivity spectra (ε* = ε′ – jε″) had a relaxation type frequency dispersion with an ill‐defined broad resonance line width of the dielectric losses (ε″). The magnetic properties of composites are very low and are independent of the filler concentration. The new nanobiocomposites are brick red in color and weakly ferromagnetic in nature. POLYM. COMPOS., 26:739–744, 2005. © 2005 Society of Plastics Engineers  相似文献   

19.
The coating of cotton fiber is used in the textile industry to increase the mechanical resistance of the yarn and their resistance to vibration, friction, impact, and elongation, which are some of the forces to which the yarn is subjected during the weaving process. The main objective of this study was to investigate the use of synthetic hydrophilic polymers, poly(vinyl alcohol) (PVA), and poly(N‐vinyl‐2‐pyrrolidone) (PVP) to coat 100% cotton textile fiber, with the aim of giving the fiber temporary mechanical resistance. For the fixation of the polymer on the fiber, UV‐C radiation was used as the crosslinking process. The influence of the crosslinking process was determined through tensile testing of the coated fibers. The results indicated that UV‐C radiation increased the mechanical resistance of the yarn coated with PVP by up to 44% and the yarn coated with PVA by up to 67% compared with the pure cotton yarn, that is, without polymeric coating and crosslinking. This study is of great relevance, and it is important to consider that UV‐C radiation dispenses with the use of chemical substances and prevents the generation of toxic waste at the end of the process. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2011  相似文献   

20.
With the density and viscosity results for five polymers—poly(vinyl alcohol) (PVA), poly(vinyl pyrrolidone) (PVP), gelatin (Ge), starch (St), and carboxymethylcellulose (CMC)—measured in aqueous solutions at different temperatures, we have computed the excess molar volumes and activities. Smaller excess molar volumes for PVA solutions are attributed to specific types of interactions, whereas for other polymers, these data are quite large, indicating dispersion‐type interactions. The activity data of the polymer solutions vary widely, depending on the nature of the polymers and their intermolecular interactions. The freestanding film properties of the polymers indicate that Ge and PVA produce stable films, whereas brittle films can be obtained for PVP and St. The mechanical strength properties of PVA and CMC have been found to be suitable for membrane fabrication. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci, 2007  相似文献   