摘    要:对高能超声稀释原位反应烧结块制备锌铝合金基复合材料过程进行了研究,简要分析了超声稀释机理。研究表明,高能超声快速稀释烧结块是声空化与声流效应协同作用的结果。空化产生的瞬时高温可促进界面区域元素扩散,瞬时高压将裸露在界面上的长棒状的TiAl3击断,打破了烧结块的网状结构,并将其周围的高致密度的Al2O3和TiB2颗粒聚集区击碎。另一方面,声流引起的强烈搅拌作用减薄了过渡层,并使短棒状的TiAl3颗粒及Al2O3、TiB2微细颗粒均匀分布在熔体中。在上述分析基础上,建立了元素扩散模型和烧结块在锌铝合金中的稀释过程模型。 

关 键 词:烧结块    声空化    声流    稀释
文章编号:1000-3851(2005)06-0037-07
收稿时间:11 24 2004 12:00AM
修稿时间:2004-11-242005-02-28

ANALYSIS OF HIGH-INTENSITY ULTRASONIC DILUTION PROCESS OF XD COMPOSITES
PAN Lei,TAO Jie,WU Shenqing,CHEN Feng,LIU Zili,CHEN Zhaofeng.ANALYSIS OF HIGH-INTENSITY ULTRASONIC DILUTION PROCESS OF XD COMPOSITES[J].Acta Materiae Compositae Sinica,2005,22(6):37-43.
Authors:PAN Lei  TAO Jie  WU Shenqing  CHEN Feng  LIU Zili  CHEN Zhaofeng
Affiliation:1.College of Materials Science and Technology,Nanjing University of Aeronautics and Astronautics,Nanjing 210016,China;2.Department of Materials Science and Engineering,Southeast University,Nanjing 210096,China
Abstract:The ultrasonic dilution mechanism was analyzed through studying the fabrication process of the Zn-Al alloy matrix composites by high-intensity ultrasonic dilution of XD composites.The results show that the mechanism of ultrasonic dilution of the XD composites is the result of the cooperative effects of the acoustic cavitation and high speed acoustic streaming in the Zn-Al alloy melt.The instantaneous high temperature caused by the acoustic cavitation can promote the element's diffusion between the interface of XD composites and the ZnAl alloy melt.The instantaneous high pressure breaks off the long rod-like TiAl_3 phase protruding along the XD composite/ Zn-Al interface,and drives the gathering particles out of the net of the rod-like TiAl_3 phase.On the other hand,the intensitive agitation caused by the acoustic streaming thins the interface area and makes the short rod-like TiAl_3 phase and fine particles(Al_2O_3 and TiB_2) homogeneously disperse in the Zn-Al alloy melt.On the basis of the results,the models of the element diffusion and dilution process of the XD composites into the Zn-Al alloy melt were established.
Keywords:XD composites  acoustic cavitation  acoustic streaming  dilution
本文献已被 CNKI 维普 万方数据 等数据库收录!
点击此处可从《复合材料学报》浏览原始摘要信息
点击此处可从《复合材料学报》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号