Abstract:An experiment was performed to remove iron ions from leach solution of low-grade copper oxide ore by hematite precipitation process. The results show that the iron removal rate is 95.2% and the contents of iron, copper and sulfur in the residue are 62.7%, 0.14% and 1.6%, respectively, under the optimal processing conditions for iron removal, including reaction temperature of 180 ℃, an initial sulfuric acid concentration of 2 g/L, reaction time of 3 h, partial pressure of oxygen at 0.3 MPa and stirring speed at 400 r/min.
王益昭, 何贵香, 付怀飞, 潘彩健, 蒋学先, 范旷生. 低品位氧化铜矿浸出液赤铁矿法除铁[J]. 矿冶工程, 2022, 42(2): 110-112.
WANG Yi-zhao, HE Gui-xiang, FU Huai-fei, PAN Cai-jian, JIANG Xue-xian, FAN Kuang-sheng. Iron Removal from Leach Solution of Low-Grade Copper Oxide Ore by Hematite Precipitation Process. Mining and Metallurgical Engineering, 2022, 42(2): 110-112.
[1] 张兴勋. 某低品位次生硫化铜矿生物柱浸试验[J]. 矿产综合利用, 2020(3):111-116.
[2] 杨秋菊,刘久清,蒋 彬,等. 高铁低铜溶液磷酸盐除铁工艺[J]. 中南大学学报(自然科学版), 2012,43(10):3763-3768.
[3] 彭 宇,肖发新,孙树臣,等. 高碱性脉石低品位氧化铜矿提铜研究进展[J]. 有色金属科学与工程, 2020,11(5):69-74.
[4] 王红军,刘久清,周 钦,等. 低品位铜矿浸出液除铁及纳滤浓缩铜的研究[J]. 中南大学学报(自然科学版), 2014,45(12):4111-4115.
[5] 陈家镛,余淑秋,伍志春. 湿法冶金中铁的分离与利用[M]. 北京:冶金工业出版社, 1991.
[6] 李存兄,魏 昶,邓志敢,等. FeSO4-H2O体系中水热赤铁矿沉铁及亚稳态铁物相转变行为[J]. 中国有色金属学报, 2018,28(3):628-636.
[7] HAN Hai-sheng, SUN Wei, HU Yue-hua, et al. Induced crystallization of goethite precipitate from nickel sulfate solution by limonite seeding[J]. Hydrometallurgy, 2017,174:253-257.
[8] 岳 明,孙宁磊,邹 兴,等. 锌浸出液三价铁直接水解赤铁矿法除铁的探讨[J]. 中国有色冶金, 2012,41(4):80-85.
[9] 邓志敢,魏 昶,朱北平,等. 工艺参数对湿法炼锌赤铁矿法沉铁行为的影响[J]. 矿冶, 2020,29(2):49-53.
[10] Ruiz M C, Zapata J, Padilla R. Effect of variables on the quality of hematite precipitated from sulfate solutions[J]. Hydrometallurgy, 2007,89(1):32-39.
[11] Li C, Deng Z, Chang W, et al. Production of low-sulfur hematite by hydrothermal oxydrolysis of ferrous sulfate[J]. Hydrometallurgy, 2018,178:294-300.
[12] Posnjak E, Merwin H E. The system, Fe2O3-SO3-H2O[J]. Journal of the American Chemical Society, 2002,44(9):1965-1994.